Cita APA (7a ed.)

Chepurov, A., Sonin, V., Shcheglov, D., Zhimulev, E., Sitnikov, S., Yelisseyev, A., & Chepurov, A. (2021). Surface Porosity of Natural Diamond Crystals after the Catalytic Hydrogenation. MDPI AG.

Cita Chicago Style (17a ed.)

Chepurov, Aleksei, Valeri Sonin, Dmitry Shcheglov, Egor Zhimulev, Sergey Sitnikov, Alexander Yelisseyev, y Anatoly Chepurov. Surface Porosity of Natural Diamond Crystals After the Catalytic Hydrogenation. MDPI AG, 2021.

Cita MLA (8a ed.)

Chepurov, Aleksei, et al. Surface Porosity of Natural Diamond Crystals After the Catalytic Hydrogenation. MDPI AG, 2021.