Studying from the Properties of Chemi-Mechanical Pulping and Alkaline Peroxide Mechanical Pulping of Wheat Straw Golestan province

In this study, mechanical and optical properties of CMP, one stage APMP and two stage APMP pulps ( from Tajan wheat straw Golestan province ) were investigated. wheat straw collected at research center of Agriculture and Natural resources of Golestan province. Fiber dimensions such as average fiber...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Saeid Kamrani, Ahmad reza Saraeyan, Eyman Akbarpoor
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2010
Materias:
Acceso en línea:https://doaj.org/article/148c8f2d2de742e0bea31ec6419b7906
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:148c8f2d2de742e0bea31ec6419b7906
record_format dspace
spelling oai:doaj.org-article:148c8f2d2de742e0bea31ec6419b79062021-12-02T09:10:58ZStudying from the Properties of Chemi-Mechanical Pulping and Alkaline Peroxide Mechanical Pulping of Wheat Straw Golestan province1735-09132383-112X10.22092/ijwpr.2010.117264https://doaj.org/article/148c8f2d2de742e0bea31ec6419b79062010-03-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_117264_6cf28adb0f703438a210fa9063fb3883.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XIn this study, mechanical and optical properties of CMP, one stage APMP and two stage APMP pulps ( from Tajan wheat straw Golestan province ) were investigated. wheat straw collected at research center of Agriculture and Natural resources of Golestan province. Fiber dimensions such as average fiber length , diameter cell , lumen and  fiber wall thickness were assessed at 1.18mm, 18.156, 11.461 and 3.396 microns, respectively. chemical  components such as cellulose , lignin , ash and extractives were assessed at 53.7, 21.1, 5.1 and 8.5 percent, respectively. Based on the preliminary experiment results, impregnation temperature was 950C, impregnation times of 10, 20, 30, 40 minutes, caustic charge 10% and peroxide charge was 3% in CMP ,one stage APMP  and two stages APMP pulps. Considering pulp properties and treatment conditions, many treatments including 20 and 40 minutes treatments were selected for making of handsheet. The selected pulps were refined up to 350 ml (CSF) freeness prior to making of hasndsheet. Final results indicated that two stages APMP pulp (impregnation in time 40 minutes) had  the highest burst strength, breaking length and brightness. Also, the results of yield and tear strength showed that, there was no meaningful difference at the 5% level between three methods CMP, one and two stages of APMP pulps.Saeid KamraniAhmad reza SaraeyanEyman AkbarpoorRegional Information Center for Science and Technology (RICeST)articleTajan wheat strawChemi-mechanical PulpingAlkaline Peroxide Mechanical PulpingMECHANICAL PROPERTIESOptical propertiesyieldForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 25, Iss 1, Pp 32-47 (2010)
institution DOAJ
collection DOAJ
language FA
topic Tajan wheat straw
Chemi-mechanical Pulping
Alkaline Peroxide Mechanical Pulping
MECHANICAL PROPERTIES
Optical properties
yield
Forestry
SD1-669.5
spellingShingle Tajan wheat straw
Chemi-mechanical Pulping
Alkaline Peroxide Mechanical Pulping
MECHANICAL PROPERTIES
Optical properties
yield
Forestry
SD1-669.5
Saeid Kamrani
Ahmad reza Saraeyan
Eyman Akbarpoor
Studying from the Properties of Chemi-Mechanical Pulping and Alkaline Peroxide Mechanical Pulping of Wheat Straw Golestan province
description In this study, mechanical and optical properties of CMP, one stage APMP and two stage APMP pulps ( from Tajan wheat straw Golestan province ) were investigated. wheat straw collected at research center of Agriculture and Natural resources of Golestan province. Fiber dimensions such as average fiber length , diameter cell , lumen and  fiber wall thickness were assessed at 1.18mm, 18.156, 11.461 and 3.396 microns, respectively. chemical  components such as cellulose , lignin , ash and extractives were assessed at 53.7, 21.1, 5.1 and 8.5 percent, respectively. Based on the preliminary experiment results, impregnation temperature was 950C, impregnation times of 10, 20, 30, 40 minutes, caustic charge 10% and peroxide charge was 3% in CMP ,one stage APMP  and two stages APMP pulps. Considering pulp properties and treatment conditions, many treatments including 20 and 40 minutes treatments were selected for making of handsheet. The selected pulps were refined up to 350 ml (CSF) freeness prior to making of hasndsheet. Final results indicated that two stages APMP pulp (impregnation in time 40 minutes) had  the highest burst strength, breaking length and brightness. Also, the results of yield and tear strength showed that, there was no meaningful difference at the 5% level between three methods CMP, one and two stages of APMP pulps.
format article
author Saeid Kamrani
Ahmad reza Saraeyan
Eyman Akbarpoor
author_facet Saeid Kamrani
Ahmad reza Saraeyan
Eyman Akbarpoor
author_sort Saeid Kamrani
title Studying from the Properties of Chemi-Mechanical Pulping and Alkaline Peroxide Mechanical Pulping of Wheat Straw Golestan province
title_short Studying from the Properties of Chemi-Mechanical Pulping and Alkaline Peroxide Mechanical Pulping of Wheat Straw Golestan province
title_full Studying from the Properties of Chemi-Mechanical Pulping and Alkaline Peroxide Mechanical Pulping of Wheat Straw Golestan province
title_fullStr Studying from the Properties of Chemi-Mechanical Pulping and Alkaline Peroxide Mechanical Pulping of Wheat Straw Golestan province
title_full_unstemmed Studying from the Properties of Chemi-Mechanical Pulping and Alkaline Peroxide Mechanical Pulping of Wheat Straw Golestan province
title_sort studying from the properties of chemi-mechanical pulping and alkaline peroxide mechanical pulping of wheat straw golestan province
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 2010
url https://doaj.org/article/148c8f2d2de742e0bea31ec6419b7906
work_keys_str_mv AT saeidkamrani studyingfromthepropertiesofchemimechanicalpulpingandalkalineperoxidemechanicalpulpingofwheatstrawgolestanprovince
AT ahmadrezasaraeyan studyingfromthepropertiesofchemimechanicalpulpingandalkalineperoxidemechanicalpulpingofwheatstrawgolestanprovince
AT eymanakbarpoor studyingfromthepropertiesofchemimechanicalpulpingandalkalineperoxidemechanicalpulpingofwheatstrawgolestanprovince
_version_ 1718398167562584064