Deashing and desulfurization of subbituminous coal from the East field (Bogovina Basin, Serbia) - insights from chemical leaching

The study is focused on the determination of the most effective chemical leaching process for the simultaneous demineralization/deashing and desulfurization of subbituminous coal from the Bogovina Basin. Coal was treated for 30 min, at different temperatures, using variable concentrations of hydroch...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Pantović-Spajić Katarina, Marković Branislav, Pavlović Miroslav M., Sokić Miroslav, Zildžović Snežana, Đorđević Nataša, Stojanović Ksenija
Formato: article
Lenguaje:EN
Publicado: Serbian Chemical Society 2021
Materias:
Acceso en línea:https://doaj.org/article/172fe9bc04224e9e9b71585bac733c20
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
Descripción
Sumario:The study is focused on the determination of the most effective chemical leaching process for the simultaneous demineralization/deashing and desulfurization of subbituminous coal from the Bogovina Basin. Coal was treated for 30 min, at different temperatures, using variable concentrations of hydrochloric, nitric, acetic and citric acids; hydrogen peroxide, mixture of hydrogen peroxide and nitric acid (pH 2), as well as by the stepwise leaching process (nitric acid + mixture of hydrogen peroxide and nitric acid, pH 2). The changes in mineral composition, caused by the chemical leaching, are followed using X-ray diffraction, whereas alterations of coal organic matter are tracked by Fourier-transform infrared spectroscopy and the content of fixed carbon. Inorganic acid leaching, regardless of the temperature and acid concentration, enabled the successful deashing of coal, whereas the percent of desulfurization was insufficient. The organic acid leaching was not satisfactory for both, deashing and desulfurization. Leaching by H2O2 and H2O2/HNO3 mixture (pH 2) resulted in moderate desulfurization, but the ash reduction was low. The most suitable method for the simultaneous effective ash (78 wt.%) and the sulfur (66 wt. %) removal from Bogovina coal is the two-step leaching, combining 10 vol. % HNO3 and mixture of 35 vol. % H2O2/10 vol. % HNO3 of pH 2 at 60°C.