The Run-in Process for Stable Friction Fade-Out and Tribofilm Analyses by SEM and Nano-Indenter
It was shown in previous reports by authors that friction coefficients of the level of 0.0001 were achieved when ZrO2 (Y-PSZ: yttria partially stabilized zirconia) pins were slid against diamond-like carbon (DLC) films in H2-gas environment under heavy applied load of 63.7 N (friction fade-out, FFO)...