Investigation on production of particleboard from Date palm residues

The influence of production variable such as residues moisture content at time of chipping or flaking, hardner and press time on properties of particleboard from date palm residues is investigated. Each variable was investigated at three different levels and a total of 24 combinations of variables w...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Ahmad Jahan latibari, Abdolrahman Hosseinzadeh, Amir Nourbakhsh, Abolfazl Kargarfard, Fardad Golbabaei
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 1996
Materias:
MOR
MOE
Acceso en línea:https://doaj.org/article/1ccf98b0290c42529c6e03883faf0721
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:1ccf98b0290c42529c6e03883faf0721
record_format dspace
spelling oai:doaj.org-article:1ccf98b0290c42529c6e03883faf07212021-12-02T05:36:34ZInvestigation on production of particleboard from Date palm residues1735-09132383-112X10.22092/ijwpr.1996.117436https://doaj.org/article/1ccf98b0290c42529c6e03883faf07211996-09-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_117436_291e31b9227632f3750c2503a4666b52.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XThe influence of production variable such as residues moisture content at time of chipping or flaking, hardner and press time on properties of particleboard from date palm residues is investigated. Each variable was investigated at three different levels and a total of 24 combinations of variables were studied. The results of this investigation indicate that:  - Residues moisture content at the time of chipping or flaking affects both physical and mechanical properties of boards. MOR and MOE of board made from flakes produced by dry chipping and either wet or dry flaking was higher than others and its dimensional stability was better. Chipping or flaking moisture did not affect IB significantly. - Hardner consumption did not significantly influence the properties, but increasing hardner consumption to 3 percent of resin content (solid basis) improved board properties. - Press time also did not influence board properties and for the production of 15 mm. boards, either 5 or 6 minutes press time can be used. -For the production of boards to satisfy DIN requirement, following variable combination can be utilized: dry chipping - wet flaking, 3 percent hardner and 6 minutes press time.Ahmad Jahan latibariAbdolrahman HosseinzadehAmir NourbakhshAbolfazl KargarfardFardad GolbabaeiRegional Information Center for Science and Technology (RICeST)articleMORMOEDate palmForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 1, Iss 1 شماره 148, Pp 50-110 (1996)
institution DOAJ
collection DOAJ
language FA
topic MOR
MOE
Date palm
Forestry
SD1-669.5
spellingShingle MOR
MOE
Date palm
Forestry
SD1-669.5
Ahmad Jahan latibari
Abdolrahman Hosseinzadeh
Amir Nourbakhsh
Abolfazl Kargarfard
Fardad Golbabaei
Investigation on production of particleboard from Date palm residues
description The influence of production variable such as residues moisture content at time of chipping or flaking, hardner and press time on properties of particleboard from date palm residues is investigated. Each variable was investigated at three different levels and a total of 24 combinations of variables were studied. The results of this investigation indicate that:  - Residues moisture content at the time of chipping or flaking affects both physical and mechanical properties of boards. MOR and MOE of board made from flakes produced by dry chipping and either wet or dry flaking was higher than others and its dimensional stability was better. Chipping or flaking moisture did not affect IB significantly. - Hardner consumption did not significantly influence the properties, but increasing hardner consumption to 3 percent of resin content (solid basis) improved board properties. - Press time also did not influence board properties and for the production of 15 mm. boards, either 5 or 6 minutes press time can be used. -For the production of boards to satisfy DIN requirement, following variable combination can be utilized: dry chipping - wet flaking, 3 percent hardner and 6 minutes press time.
format article
author Ahmad Jahan latibari
Abdolrahman Hosseinzadeh
Amir Nourbakhsh
Abolfazl Kargarfard
Fardad Golbabaei
author_facet Ahmad Jahan latibari
Abdolrahman Hosseinzadeh
Amir Nourbakhsh
Abolfazl Kargarfard
Fardad Golbabaei
author_sort Ahmad Jahan latibari
title Investigation on production of particleboard from Date palm residues
title_short Investigation on production of particleboard from Date palm residues
title_full Investigation on production of particleboard from Date palm residues
title_fullStr Investigation on production of particleboard from Date palm residues
title_full_unstemmed Investigation on production of particleboard from Date palm residues
title_sort investigation on production of particleboard from date palm residues
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 1996
url https://doaj.org/article/1ccf98b0290c42529c6e03883faf0721
work_keys_str_mv AT ahmadjahanlatibari investigationonproductionofparticleboardfromdatepalmresidues
AT abdolrahmanhosseinzadeh investigationonproductionofparticleboardfromdatepalmresidues
AT amirnourbakhsh investigationonproductionofparticleboardfromdatepalmresidues
AT abolfazlkargarfard investigationonproductionofparticleboardfromdatepalmresidues
AT fardadgolbabaei investigationonproductionofparticleboardfromdatepalmresidues
_version_ 1718400280078319616