Fatigue strength evaluation of a 13%Cr supermartensitic stainless steel by the thermographic method
The fatigue limits of a 13Cr super-martensitic stainless steel from a hot rolled seamless tube were determined for three heat treatment conditions, including the as received quenched and tempered (QT) condition, quenched (Q), and quenched and double tempered (Q-DT). These heat treatments were applie...
Guardado en:
Autores principales: | Tavares Sérgio S.M., Abib Bruna, Kenedi Paulo, Alves Odivaldo C., Almeida Brígida B. |
---|---|
Formato: | article |
Lenguaje: | EN FR |
Publicado: |
EDP Sciences
2021
|
Materias: | |
Acceso en línea: | https://doaj.org/article/1e9b9d414d3049b0907bb9f80f5b7953 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Characterization and performance of high strength steel 51CrV4 under cyclic loading
por: Malikoutsakis Michail, et al.
Publicado: (2021) -
Rolling and Rolling-Sliding Contact Fatigue Failure Mechanisms in 32 CrMoV 13 Nitrided Steel—An Experimental Study
por: Luís Coelho, et al.
Publicado: (2021) -
Effect of Sandblasting on Static and Fatigue Strength of Flash Butt Welded 75Cr4 Bandsaw Blades
por: Andrzej Kubit, et al.
Publicado: (2021) -
Low-cycle fatigue behavior of stainless-steel elbows having local wall thinning
por: Yasuhiro ASHIBA, et al.
Publicado: (2020) -
Improvement of Microhardness and Corrosion Resistance of Stainless Steel by Nanocomposite Coating
por: Hiba Husam Ismail, et al.
Publicado: (2014)