Fatigue strength evaluation of a 13%Cr supermartensitic stainless steel by the thermographic method
The fatigue limits of a 13Cr super-martensitic stainless steel from a hot rolled seamless tube were determined for three heat treatment conditions, including the as received quenched and tempered (QT) condition, quenched (Q), and quenched and double tempered (Q-DT). These heat treatments were applie...