An efficient and environmentally friendly route for PbS crystal recovery from lead ash generated in tin removal section (LATR) via high-speed leaching and recrystallization method

This paper mainly investigated the synthesis of a high purity PbS crystal directly from lead ash which was collected from Tin ash removal process (LATR). The LATR was firstly disposed by nitric acid leaching system to generate the lead nitrate solution. The PbS crystal was prepared by mixing the lea...