Pulping and paper making properties of Populus costanzo

In this Investigation chemical, physical, morphology, pulp and paper making characteristics of   Populus costanzo were studied. The average dry and critical specific gravity was found to be  0.39and 0.36 and the fiber morphology including fiber length  , diameter ,lumen and thickness of cell wall 1....

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Abas Fakhryan, Hossein Hosseinkhani, Fardad Golbabaei, Mohammad mehdi Brazandeh
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2010
Materias:
Acceso en línea:https://doaj.org/article/20c18f5f8c42425ba157db53fa94638b
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
Descripción
Sumario:In this Investigation chemical, physical, morphology, pulp and paper making characteristics of   Populus costanzo were studied. The average dry and critical specific gravity was found to be  0.39and 0.36 and the fiber morphology including fiber length  , diameter ,lumen and thickness of cell wall 1.14 mm,28.84 µm, 28 µm ,and 2.92 µm was determined respectively. The average chemical composition including cellulose 50.74%, lignin 19.18%, Ext. 1.22%  and Ash 1.65% were measured. In order to cook and pulping, Kraft process was used. The maximum  yield and kappa number of Populus costanzo at 1 hour cooking time, 150°c cooking temperature and 12% effective alkali condition  obtained at 61.91% and 54.83 respectively and the minimum  yield and kappa number at 3 hour cooking time, 170°c cooking temperature and 16% effective alkali condition  obtained at 45.63% and 13.42 respectively.