Effect of steaming time on medium density fiberboard properties produced from beech wood fibers
In this investigation, 36 laboratory Medium Density Fiberboard (MDF) panels were produced using beech wood fibers. Variables were three steaming time (5, 10 and 15 minutes), two press time (4 and 6 minutes) and two resin consumption levels (9 and 11%). The physical and mechanical properties of panel...
Guardado en:
Autores principales: | Abolfazl Kargarfard, Reza Hajihassani, Fatemeh Rezaei |
---|---|
Formato: | article |
Lenguaje: | FA |
Publicado: |
Regional Information Center for Science and Technology (RICeST)
2011
|
Materias: | |
Acceso en línea: | https://doaj.org/article/26877fd3d52b49d3b17a44cf51d2b436 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
The potential of utilization of alder wood fibers In medium density fiberboard production
por: Abolfazl Kargarfard, et al.
Publicado: (2010) -
Investigation on physical and mechanical properties of medium density
fiberboard produced from Eucalyptus steriaticalyx fibers
por: Abolfazl Kargarfard
Publicado: (2012) -
Investigation on Physical and Mechanical Properties of Medium Density Fiberboard Produced From Eucalyptus camaldulensis Fibers
por: Abolfazl Kargarfard, et al.
Publicado: (2010) -
The Investigation of Press Temperature and Time on Properties of Medium Density Fiberboard Produced From Cotton Stalks Fibers
por: Abolfazl Kargarfard, et al.
Publicado: (2016) -
The effect of press temperature and press time on Medium Density Fiberboard (MDF) properties produced from EucalyptusIntertexta fibers
por: Abolfazl Kargarfard, et al.
Publicado: (2009)