The effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene
Abstract The effect of adding steamed and non-steamed fiber on physical and mechanical properties of the composites made of recycled polypropylene was investigated. Recycled polypropylene was used as a basic matrix at a 57% level, and poplar fibers were used at 180 °C for 1 h at a constant level of...
Guardado en:
Autores principales: | , |
---|---|
Formato: | article |
Lenguaje: | FA |
Publicado: |
Regional Information Center for Science and Technology (RICeST)
2017
|
Materias: | |
Acceso en línea: | https://doaj.org/article/2a06a8dabb494ca4bd69f48ca3542fb4 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
id |
oai:doaj.org-article:2a06a8dabb494ca4bd69f48ca3542fb4 |
---|---|
record_format |
dspace |
spelling |
oai:doaj.org-article:2a06a8dabb494ca4bd69f48ca3542fb42021-12-02T02:37:10ZThe effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene1735-09132383-112X10.22092/ijwpr.2017.108571.1372https://doaj.org/article/2a06a8dabb494ca4bd69f48ca3542fb42017-10-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_113053_4b3fe39fc525a00e13297dc73e75e1f2.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XAbstract The effect of adding steamed and non-steamed fiber on physical and mechanical properties of the composites made of recycled polypropylene was investigated. Recycled polypropylene was used as a basic matrix at a 57% level, and poplar fibers were used at 180 °C for 1 h at a constant level of 40% in two forms: non-steamed and steamed. The ratio of steamed fibers to non-steamed fibers in composites was 100:0, 50:50, and 0:100, respectively. For all components, the coupling agent was maleic anhydride at a level of 3%. Mixing was done using an internal mixer at 180 °C and 60 rpm, and the samples were constructed by injection molding method. To investigate the effect of steam treatment on the fiber structure and crystallization, X-ray diffraction analysis and FTIR spectra were used. The results showed that the Steaming had no significant effect on resistance. But with steaming increased mechanical properties and physical properties of reduced. Keywords: Composites, Recycled polypropylene, Steamed fiber, XRD, FTIRAhmad SamarihaHabibollah Khademi EslamRegional Information Center for Science and Technology (RICeST)articleCOMPOSITESRecycled polypropyleneSteamed fiberXRDFTIRForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 32, Iss 3, Pp 411-421 (2017) |
institution |
DOAJ |
collection |
DOAJ |
language |
FA |
topic |
COMPOSITES Recycled polypropylene Steamed fiber XRD FTIR Forestry SD1-669.5 |
spellingShingle |
COMPOSITES Recycled polypropylene Steamed fiber XRD FTIR Forestry SD1-669.5 Ahmad Samariha Habibollah Khademi Eslam The effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene |
description |
Abstract The effect of adding steamed and non-steamed fiber on physical and mechanical properties of the composites made of recycled polypropylene was investigated. Recycled polypropylene was used as a basic matrix at a 57% level, and poplar fibers were used at 180 °C for 1 h at a constant level of 40% in two forms: non-steamed and steamed. The ratio of steamed fibers to non-steamed fibers in composites was 100:0, 50:50, and 0:100, respectively. For all components, the coupling agent was maleic anhydride at a level of 3%. Mixing was done using an internal mixer at 180 °C and 60 rpm, and the samples were constructed by injection molding method. To investigate the effect of steam treatment on the fiber structure and crystallization, X-ray diffraction analysis and FTIR spectra were used. The results showed that the Steaming had no significant effect on resistance. But with steaming increased mechanical properties and physical properties of reduced. Keywords: Composites, Recycled polypropylene, Steamed fiber, XRD, FTIR |
format |
article |
author |
Ahmad Samariha Habibollah Khademi Eslam |
author_facet |
Ahmad Samariha Habibollah Khademi Eslam |
author_sort |
Ahmad Samariha |
title |
The effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene |
title_short |
The effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene |
title_full |
The effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene |
title_fullStr |
The effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene |
title_full_unstemmed |
The effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene |
title_sort |
effect of water vapor treatment of wood flour on physical and mechanical properties of hybrid composite made of poplar fiber and recycled polypropylene |
publisher |
Regional Information Center for Science and Technology (RICeST) |
publishDate |
2017 |
url |
https://doaj.org/article/2a06a8dabb494ca4bd69f48ca3542fb4 |
work_keys_str_mv |
AT ahmadsamariha theeffectofwatervaportreatmentofwoodflouronphysicalandmechanicalpropertiesofhybridcompositemadeofpoplarfiberandrecycledpolypropylene AT habibollahkhademieslam theeffectofwatervaportreatmentofwoodflouronphysicalandmechanicalpropertiesofhybridcompositemadeofpoplarfiberandrecycledpolypropylene AT ahmadsamariha effectofwatervaportreatmentofwoodflouronphysicalandmechanicalpropertiesofhybridcompositemadeofpoplarfiberandrecycledpolypropylene AT habibollahkhademieslam effectofwatervaportreatmentofwoodflouronphysicalandmechanicalpropertiesofhybridcompositemadeofpoplarfiberandrecycledpolypropylene |
_version_ |
1718402336528793600 |