Amorphous Thermal Spray Coating with Hard Materials Exhibiting Cleavage Fracture
Hard materials were mixed with alloy powders and thermally sprayed at an ultra rapid cooling rate of more than 106°C/s. For example, 65Ni15Cr16P4B at% alloy powder containing tungsten carbide was thermally sprayed. SEM image showed tungsten carbide paticles were scattered in the amorphous alloy coat...
Guardado en:
Autores principales: | Toshiharu Morimoto, Yoshio Shin, Takashi Kumai, Jun Yanagimoto |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
Japanese Society of Tribologists
2015
|
Materias: | |
Acceso en línea: | https://doaj.org/article/2b1c968105eb44fd91a363272dfb9fd4 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Composition optimization of amorphous AlNiZr alloys
por: Zhibin ZHANG, et al.
Publicado: (2021) -
ANALYSIS AND STUDY OF AMORPHOUS ALLOYS PROPERTIES
por: T.P. Pavlenko, et al.
Publicado: (2013) -
Demonstration of Wear Monitoring of Amorphous Carbon Films with Epoxy Resin Underlayer Containing Phosphor
por: Atsawin Salee, et al.
Publicado: (2013) -
Effect of Fe addition on glass-forming ability, thermal stability of B2 CuZr phase and crystallization kinetics for CuZr-based amorphous alloys
por: Ziyan Hao, et al.
Publicado: (2021) -
Preparation of Wear-Resistant Coating on Ti6Al4V Alloy by Cold Spraying and Plasma Electrolytic Oxidation
por: Mingzeng Shao, et al.
Publicado: (2021)