Abstract Zirconium carbide (ZrC) reinforced tungsten (W) composite was hot-pressed at 2200 °C for 1 h in vacuum, which was subsequently heat treated in the temperature range of 2200 to 2500 °C for 1.5 or 2 h. The relative ratios of ZrC phase were 21.0, 23.3 and 25.9 mol.% for the mixture of starting...