Determination of Friction Performance of High Friction Surface Treatment Based on Alternative Macrotexture Metric

Surface friction is currently the most common metric for evaluating the performance of high friction surface treatment (HFST). However, friction test methods such as the locked wheel skid tester (LWST) commonly provide a spot measurement. Large variations may arise in the LWST testing on curves. Bas...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Hua Zhao, Fulu Wei, Ce Wang, Shuo Li, Jie Shan
Formato: article
Lenguaje:EN
Publicado: MDPI AG 2021
Materias:
T
Acceso en línea:https://doaj.org/article/3378b65437d64c3f8ef3c7c1b70ea5e4
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
Descripción
Sumario:Surface friction is currently the most common metric for evaluating the performance of high friction surface treatment (HFST). However, friction test methods such as the locked wheel skid tester (LWST) commonly provide a spot measurement. Large variations may arise in the LWST testing on curves. Based on 21 actual HFST projects, a study was performed to use a macrotexture metric, i.e., the mean profile depth (MPD) to evaluate HFST’s performance and improve its quality control (QC)/quality assurance (QA) procedures. The material properties were presented to understand the aspects of HFST. The method for calculating MPD was modified to account for the variations of macrotexture measurements. A vehicle-based test system was utilized to measure MPD periodically over an 18-month period since HFST installation. Statistical analysis was performed on the MPD measurements to identify the effects of influencing factors. Compared with the friction from LWST, MPD was equally effective in evaluating HFST performance. However, the use of MPD eliminated the errors as arisen in LWST testing and made it possible to detect surface distresses, including aggregate loss, delamination, and cracking. The expected overall MPD may be calculated by combining the MPD measurements made three months after installation at different HFST sites and used as a metric for evaluating HFST performance and QC/QA.