Melting of high-carbon ferrochrome using coal of the saryadyr deposit
The article presents the results of large-scale laboratory tests on the smelting of high-carbon ferrochrome with the replacement of parts metallurgical coke with high-ash coal from the Saryadyr deposits. According to the test results, it can be stated that the optimal percentage of replacing metallu...
Guardado en:
Autores principales: | , , , , , |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
Croatian Metallurgical Society
2022
|
Materias: | |
Acceso en línea: | https://doaj.org/article/38561de82b8e458b8e93131b59472776 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
id |
oai:doaj.org-article:38561de82b8e458b8e93131b59472776 |
---|---|
record_format |
dspace |
spelling |
oai:doaj.org-article:38561de82b8e458b8e93131b594727762021-11-28T20:07:56ZMelting of high-carbon ferrochrome using coal of the saryadyr deposit0543-58461334-2576https://doaj.org/article/38561de82b8e458b8e93131b594727762022-01-01T00:00:00Zhttps://hrcak.srce.hr/file/386166https://doaj.org/toc/0543-5846https://doaj.org/toc/1334-2576The article presents the results of large-scale laboratory tests on the smelting of high-carbon ferrochrome with the replacement of parts metallurgical coke with high-ash coal from the Saryadyr deposits. According to the test results, it can be stated that the optimal percentage of replacing metallurgical coke with high-ash Saradyr coal is 30 – 40 %. During a large-scale laboratory test, it was also established that the cost of the alloy was reduced due to the partial replacement of expensive coke and removes the fluxing component of quartzite from the charge composition, and improves the TPE of the high-carbon ferrochrome smelting process.Ye. KuatbayA. NurumgaliyevYe. ShabanovO. ZayakinS. GabdullinT. ZhuniskaliyevCroatian Metallurgical Societyarticlechrome orehigh ash coalreductioncarbonaceous reductantthermal ore furnaceMining engineering. MetallurgyTN1-997ENMetalurgija, Vol 61, Iss 2, Pp 367-370 (2022) |
institution |
DOAJ |
collection |
DOAJ |
language |
EN |
topic |
chrome ore high ash coal reduction carbonaceous reductant thermal ore furnace Mining engineering. Metallurgy TN1-997 |
spellingShingle |
chrome ore high ash coal reduction carbonaceous reductant thermal ore furnace Mining engineering. Metallurgy TN1-997 Ye. Kuatbay A. Nurumgaliyev Ye. Shabanov O. Zayakin S. Gabdullin T. Zhuniskaliyev Melting of high-carbon ferrochrome using coal of the saryadyr deposit |
description |
The article presents the results of large-scale laboratory tests on the smelting of high-carbon ferrochrome with the replacement of parts metallurgical coke with high-ash coal from the Saryadyr deposits. According to the test results, it can be stated that the optimal percentage of replacing metallurgical coke with high-ash Saradyr coal is 30 – 40 %. During a large-scale laboratory test, it was also established that the cost of the alloy was reduced due to the partial replacement of expensive coke and removes the fluxing component of quartzite from the charge composition, and improves the TPE of the high-carbon ferrochrome smelting process. |
format |
article |
author |
Ye. Kuatbay A. Nurumgaliyev Ye. Shabanov O. Zayakin S. Gabdullin T. Zhuniskaliyev |
author_facet |
Ye. Kuatbay A. Nurumgaliyev Ye. Shabanov O. Zayakin S. Gabdullin T. Zhuniskaliyev |
author_sort |
Ye. Kuatbay |
title |
Melting of high-carbon ferrochrome using coal of the saryadyr deposit |
title_short |
Melting of high-carbon ferrochrome using coal of the saryadyr deposit |
title_full |
Melting of high-carbon ferrochrome using coal of the saryadyr deposit |
title_fullStr |
Melting of high-carbon ferrochrome using coal of the saryadyr deposit |
title_full_unstemmed |
Melting of high-carbon ferrochrome using coal of the saryadyr deposit |
title_sort |
melting of high-carbon ferrochrome using coal of the saryadyr deposit |
publisher |
Croatian Metallurgical Society |
publishDate |
2022 |
url |
https://doaj.org/article/38561de82b8e458b8e93131b59472776 |
work_keys_str_mv |
AT yekuatbay meltingofhighcarbonferrochromeusingcoalofthesaryadyrdeposit AT anurumgaliyev meltingofhighcarbonferrochromeusingcoalofthesaryadyrdeposit AT yeshabanov meltingofhighcarbonferrochromeusingcoalofthesaryadyrdeposit AT ozayakin meltingofhighcarbonferrochromeusingcoalofthesaryadyrdeposit AT sgabdullin meltingofhighcarbonferrochromeusingcoalofthesaryadyrdeposit AT tzhuniskaliyev meltingofhighcarbonferrochromeusingcoalofthesaryadyrdeposit |
_version_ |
1718407763093094400 |