Fundamental Evaluation of Sealability of Greased Metal-to-Metal Seal on Premium Threaded Joints at High Pressure and High Temperature

Metal-to-metal seals in premium threaded joints (PJs) for Oil Country Tubular Goods are used in severe environments such as high pressure and high temperature. Under the extreme conditions, the thermal degradation of applied grease on the seal surfaces can affect the sealability of metal-to-metal se...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Keita Inose, Masaaki Sugino, Joichi Sugimura
Formato: article
Lenguaje:EN
Publicado: Japanese Society of Tribologists 2021
Materias:
Acceso en línea:https://doaj.org/article/3d9e89facaa44e188553c3299a7d17fb
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:3d9e89facaa44e188553c3299a7d17fb
record_format dspace
spelling oai:doaj.org-article:3d9e89facaa44e188553c3299a7d17fb2021-11-05T09:31:11ZFundamental Evaluation of Sealability of Greased Metal-to-Metal Seal on Premium Threaded Joints at High Pressure and High Temperature1881-219810.2474/trol.16.192https://doaj.org/article/3d9e89facaa44e188553c3299a7d17fb2021-09-01T00:00:00Zhttps://www.jstage.jst.go.jp/article/trol/16/3/16_192/_pdf/-char/enhttps://doaj.org/toc/1881-2198Metal-to-metal seals in premium threaded joints (PJs) for Oil Country Tubular Goods are used in severe environments such as high pressure and high temperature. Under the extreme conditions, the thermal degradation of applied grease on the seal surfaces can affect the sealability of metal-to-metal seal. In this study, changes in the sealability of greased metal-to-metal seal due to elevated temperature were investigated by fundamental gas tightness tests. In addition, changes in grease property at high temperature were also investigated. It was found that one of the causes of the loss of the sealability of metal-to-metal seal at high temperature was the decrease in grease viscous resistance against high pressure due to thermal degradation of grease. The decrease in grease viscous resistance was caused by the decrease in the kinematic viscosity of the base oil under 125°C at which the network structure of the thickener was almost maintained. Beyond 150°C, the decrease of complex viscosity of the grease due to the collapse of the network structure of the thickener decreased the grease viscous resistance. The latter significantly affected the loss of sealability of the metal-to-metal seal.Keita InoseMasaaki SuginoJoichi SugimuraJapanese Society of Tribologistsarticlepremium threaded jointmetal-to-metal sealgreasehigh pressurehigh temperaturegas tightnessPhysicsQC1-999Engineering (General). Civil engineering (General)TA1-2040Mechanical engineering and machineryTJ1-1570ChemistryQD1-999ENTribology Online, Vol 16, Iss 3, Pp 192-198 (2021)
institution DOAJ
collection DOAJ
language EN
topic premium threaded joint
metal-to-metal seal
grease
high pressure
high temperature
gas tightness
Physics
QC1-999
Engineering (General). Civil engineering (General)
TA1-2040
Mechanical engineering and machinery
TJ1-1570
Chemistry
QD1-999
spellingShingle premium threaded joint
metal-to-metal seal
grease
high pressure
high temperature
gas tightness
Physics
QC1-999
Engineering (General). Civil engineering (General)
TA1-2040
Mechanical engineering and machinery
TJ1-1570
Chemistry
QD1-999
Keita Inose
Masaaki Sugino
Joichi Sugimura
Fundamental Evaluation of Sealability of Greased Metal-to-Metal Seal on Premium Threaded Joints at High Pressure and High Temperature
description Metal-to-metal seals in premium threaded joints (PJs) for Oil Country Tubular Goods are used in severe environments such as high pressure and high temperature. Under the extreme conditions, the thermal degradation of applied grease on the seal surfaces can affect the sealability of metal-to-metal seal. In this study, changes in the sealability of greased metal-to-metal seal due to elevated temperature were investigated by fundamental gas tightness tests. In addition, changes in grease property at high temperature were also investigated. It was found that one of the causes of the loss of the sealability of metal-to-metal seal at high temperature was the decrease in grease viscous resistance against high pressure due to thermal degradation of grease. The decrease in grease viscous resistance was caused by the decrease in the kinematic viscosity of the base oil under 125°C at which the network structure of the thickener was almost maintained. Beyond 150°C, the decrease of complex viscosity of the grease due to the collapse of the network structure of the thickener decreased the grease viscous resistance. The latter significantly affected the loss of sealability of the metal-to-metal seal.
format article
author Keita Inose
Masaaki Sugino
Joichi Sugimura
author_facet Keita Inose
Masaaki Sugino
Joichi Sugimura
author_sort Keita Inose
title Fundamental Evaluation of Sealability of Greased Metal-to-Metal Seal on Premium Threaded Joints at High Pressure and High Temperature
title_short Fundamental Evaluation of Sealability of Greased Metal-to-Metal Seal on Premium Threaded Joints at High Pressure and High Temperature
title_full Fundamental Evaluation of Sealability of Greased Metal-to-Metal Seal on Premium Threaded Joints at High Pressure and High Temperature
title_fullStr Fundamental Evaluation of Sealability of Greased Metal-to-Metal Seal on Premium Threaded Joints at High Pressure and High Temperature
title_full_unstemmed Fundamental Evaluation of Sealability of Greased Metal-to-Metal Seal on Premium Threaded Joints at High Pressure and High Temperature
title_sort fundamental evaluation of sealability of greased metal-to-metal seal on premium threaded joints at high pressure and high temperature
publisher Japanese Society of Tribologists
publishDate 2021
url https://doaj.org/article/3d9e89facaa44e188553c3299a7d17fb
work_keys_str_mv AT keitainose fundamentalevaluationofsealabilityofgreasedmetaltometalsealonpremiumthreadedjointsathighpressureandhightemperature
AT masaakisugino fundamentalevaluationofsealabilityofgreasedmetaltometalsealonpremiumthreadedjointsathighpressureandhightemperature
AT joichisugimura fundamentalevaluationofsealabilityofgreasedmetaltometalsealonpremiumthreadedjointsathighpressureandhightemperature
_version_ 1718444282191282176