Corrosion and Galvanic behavior of Copper, Carbon steel and Zinc Couples in (3.5 %wt) Nacl Solution
The galvanic corrosion of the (Cu - Fe), (Cu - Zn) and (Fe - Zn) couples have been investigated in 3.5% NaCl solution, 40ºC, different velocities (Re = 5000, 10000 and 15000) and different area ratio’s of cathode to anode (AR= 0.5,1 and 2), by using commercial metal pipe (cylindrical tube).The Zero...
Guardado en:
Autores principales: | Jamal M. Ali, Qasim M. Abbas |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
Al-Khwarizmi College of Engineering – University of Baghdad
2009
|
Materias: | |
Acceso en línea: | https://doaj.org/article/3e5ad8e1157148d2be349002a7b93182 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Corrosion and Galvanic behavior of Copper, Carbon steeland Zinc Couples in (3.5 %wt) Nacl Solution
por: Qasim M. Abbas, et al.
Publicado: (2009) -
Corrosion Inhibition Properties of Thiazolidinedione Derivatives for Copper in 3.5 wt.% NaCl Medium
por: Hassane Lgaz, et al.
Publicado: (2021) -
Effect of Shot Peening on Fatigue Properties for Corroded and Uncorroded (CK35) Steel
por: Marwan N. Arbilei, et al.
Publicado: (2019) -
Kinetic Study of Post Combustion CO2 Absorption by Methyldiethanolamine 30 wt.% and Hexylamine 10 wt.% as New Aqueous Solution
por: Léa Mailhol, et al.
Publicado: (2021) -
Improvement of Microhardness and Corrosion Resistance of Stainless Steel by Nanocomposite Coating
por: Hiba Husam Ismail, et al.
Publicado: (2014)