Investigating the bending strength of wooden pin in H-shaped joints in MDF

Aim of this study were to examine the effects of pin diameter (6, 8 and 10 millimeter), the pins interval ( 30,50 and 70 millimeter), wooden pin penetration depth (2d,3d and 4d D=Diameter of pin) and the shape of H joint on bending strength of the joint. In order to make the H joints, the dimension...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: amir lashgari, Mohssen Ahmadi
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2012
Materias:
MDF
PVA
Acceso en línea:https://doaj.org/article/44d531b93b924aee85285897cca3369f
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:44d531b93b924aee85285897cca3369f
record_format dspace
spelling oai:doaj.org-article:44d531b93b924aee85285897cca3369f2021-12-02T06:12:11ZInvestigating the bending strength of wooden pin in H-shaped joints in MDF1735-09132383-112X10.22092/ijwpr.2012.116106https://doaj.org/article/44d531b93b924aee85285897cca3369f2012-09-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_116106_8a80d7eb78a48f806a28dc5eb1bfe437.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XAim of this study were to examine the effects of pin diameter (6, 8 and 10 millimeter), the pins interval ( 30,50 and 70 millimeter), wooden pin penetration depth (2d,3d and 4d D=Diameter of pin) and the shape of H joint on bending strength of the joint. In order to make the H joints, the dimension of the middle member was selected as 200x125x16 millimeter and the dimension of the side members were selected as 250x125x16 millimeter. MDF was used to make the joints. The wooden pin used in the present research was made from hornbeam (Carpinus betulus) which is common pin in the market. PVA glue was used to make pin joints. Twenty seven treatments were obtained out of various combinations of the variables and considering four replication for each treatment, 108 H-shaped samples were prepared. The bending strength of the joints was measured. The results from mechanical test indicated that for each pin penetration depths in H  joint, increasing the distance between pins, the bending strength decreased. Maximum bending strength was related to the pins having diameter of 10 millimeter. In 4d penetration depth, for each three diameters of 6, 8 and 10 millimeter, the maximum bending strength was reached on 30 millimeter intervals. The minimum bending strength for the pin having 6 millimeter diameter was obtained in the interval of 10 millimeter. The same results were obtained for the 2d and 3d penetration depths.amir lashgariMohssen AhmadiRegional Information Center for Science and Technology (RICeST)articledowel jointwooden pinH- jointBending strengthMDFPVAForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 27, Iss 3, Pp 423-433 (2012)
institution DOAJ
collection DOAJ
language FA
topic dowel joint
wooden pin
H- joint
Bending strength
MDF
PVA
Forestry
SD1-669.5
spellingShingle dowel joint
wooden pin
H- joint
Bending strength
MDF
PVA
Forestry
SD1-669.5
amir lashgari
Mohssen Ahmadi
Investigating the bending strength of wooden pin in H-shaped joints in MDF
description Aim of this study were to examine the effects of pin diameter (6, 8 and 10 millimeter), the pins interval ( 30,50 and 70 millimeter), wooden pin penetration depth (2d,3d and 4d D=Diameter of pin) and the shape of H joint on bending strength of the joint. In order to make the H joints, the dimension of the middle member was selected as 200x125x16 millimeter and the dimension of the side members were selected as 250x125x16 millimeter. MDF was used to make the joints. The wooden pin used in the present research was made from hornbeam (Carpinus betulus) which is common pin in the market. PVA glue was used to make pin joints. Twenty seven treatments were obtained out of various combinations of the variables and considering four replication for each treatment, 108 H-shaped samples were prepared. The bending strength of the joints was measured. The results from mechanical test indicated that for each pin penetration depths in H  joint, increasing the distance between pins, the bending strength decreased. Maximum bending strength was related to the pins having diameter of 10 millimeter. In 4d penetration depth, for each three diameters of 6, 8 and 10 millimeter, the maximum bending strength was reached on 30 millimeter intervals. The minimum bending strength for the pin having 6 millimeter diameter was obtained in the interval of 10 millimeter. The same results were obtained for the 2d and 3d penetration depths.
format article
author amir lashgari
Mohssen Ahmadi
author_facet amir lashgari
Mohssen Ahmadi
author_sort amir lashgari
title Investigating the bending strength of wooden pin in H-shaped joints in MDF
title_short Investigating the bending strength of wooden pin in H-shaped joints in MDF
title_full Investigating the bending strength of wooden pin in H-shaped joints in MDF
title_fullStr Investigating the bending strength of wooden pin in H-shaped joints in MDF
title_full_unstemmed Investigating the bending strength of wooden pin in H-shaped joints in MDF
title_sort investigating the bending strength of wooden pin in h-shaped joints in mdf
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 2012
url https://doaj.org/article/44d531b93b924aee85285897cca3369f
work_keys_str_mv AT amirlashgari investigatingthebendingstrengthofwoodenpininhshapedjointsinmdf
AT mohssenahmadi investigatingthebendingstrengthofwoodenpininhshapedjointsinmdf
_version_ 1718399987347357696