An experimental study on hole quality and different delamination approaches in the drilling of CARALL, a new FML composite
In this study, the hole quality was investigated in the drilling of CARALL composite. In addition, the delamination factor calculation approaches of Chen, Davim, and Machado were compared in terms of the delamination damage at the hole entrance surface. Chen's approach is based on the conventio...
Guardado en:
Autores principales: | Ekici Ergün, Motorcu Ali Riza, Yıldırım Ensar |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
University of Belgrade - Faculty of Mechanical Engineering, Belgrade
2021
|
Materias: | |
Acceso en línea: | https://doaj.org/article/465067d0c1df40bd906db27b42d8b32b |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Interlaminar shear strength (ILSS) characterization of fiber metal laminates (FMLs) manufactured through VARTM process
por: Muhammad Yasir Khalid, et al.
Publicado: (2021) -
On the deformation of laminated composite and sandwich curved beams
por: Avhad Pravin V., et al.
Publicado: (2021) -
Finite element investigation of lamination-induced curl due to residual stresses
por: Manogna Jambhapuram, et al.
Publicado: (2021) -
Optimization for drilling process of metal-composite aeronautical structures
por: Devitte Cristiano, et al.
Publicado: (2021) -
Compressive bearing capacity and failure mechanism of CFRP–aluminum laminate column with single-channel cross section
por: Huang Teng, et al.
Publicado: (2021)