Comparison of a 2-Dimensional Wear Scar Measurement and a 3-Dimensional Profilometer Measurement of the Same Wear Scar in a Point Contact
In a tribological experiment, one relies on the ability to measure accurately the wear scar in the contact. Usually, in a point contact, the wear scar diameter (WSD) is measured, and measurements of this kind may be compared for several different oils, for example. This type of experiment might be c...
Guardado en:
Autores principales: | Elaine S. Yamaguchi, Shenghua Li, Kam-Sik Ng |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
Japanese Society of Tribologists
2012
|
Materias: | |
Acceso en línea: | https://doaj.org/article/49e712ac47ff4e459b2899bcd15ba966 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Friction and Wear Measurements with an Adapted Ball-On-Pyramid Test Setup
por: Viktor Krasmik, et al.
Publicado: (2016) -
Development of Three-Dimensional Non-Contact Surface Profilometer and Application to Evaluation of Impact Erosion of Metal Matrix Composites
por: Yoshiro Iwai, et al.
Publicado: (2008) -
Acoustic Emission Signals and Wear Phenomena on Severe-Mild Wear Transition
por: Alan Hase, et al.
Publicado: (2008) -
Friction and Wear Properties of Sintered Cu Alloy Impregnated with Thermo-Reversible Gel-Lubricant
por: Naoki Yamano, et al.
Publicado: (2010) -
Generation of Ammonia during Wear Processes in Adhesive Wear of Titanium
por: Hiroshi Mishina, et al.
Publicado: (2015)