Evaluation of cast defects in ship propeller of recycled aluminum alloy
The material used is recycled aluminum alloy. The ship’s propeller is cast through a steel mold. The macroporosity, misrun, and cold shut defects formed in the cast products of the ship’s propellers were observed for their location, geometric shape, and size. Defects are generally formed at the tip...
Guardado en:
Autores principales: | , , , , |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
Croatian Metallurgical Society
2022
|
Materias: | |
Acceso en línea: | https://doaj.org/article/53a3ea82a55f4709b15b36cbf78bdd55 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
id |
oai:doaj.org-article:53a3ea82a55f4709b15b36cbf78bdd55 |
---|---|
record_format |
dspace |
spelling |
oai:doaj.org-article:53a3ea82a55f4709b15b36cbf78bdd552021-11-28T20:03:41ZEvaluation of cast defects in ship propeller of recycled aluminum alloy0543-58461334-2576https://doaj.org/article/53a3ea82a55f4709b15b36cbf78bdd552022-01-01T00:00:00Zhttps://hrcak.srce.hr/file/386150https://doaj.org/toc/0543-5846https://doaj.org/toc/1334-2576The material used is recycled aluminum alloy. The ship’s propeller is cast through a steel mold. The macroporosity, misrun, and cold shut defects formed in the cast products of the ship’s propellers were observed for their location, geometric shape, and size. Defects are generally formed at the tip of the blade with various geometries and sizes, and shrinkage cavity defects are observed at the butt of the blade. No defects were found in the product when die mold was preheated.Akhyar .I. HasanuddinM. IbrahimA. FarhanZ. JalilCroatian Metallurgical Societyarticlealuminum alloypropellercastingdefectmacroporosityMining engineering. MetallurgyTN1-997ENMetalurgija, Vol 61, Iss 2, Pp 309-312 (2022) |
institution |
DOAJ |
collection |
DOAJ |
language |
EN |
topic |
aluminum alloy propeller casting defect macroporosity Mining engineering. Metallurgy TN1-997 |
spellingShingle |
aluminum alloy propeller casting defect macroporosity Mining engineering. Metallurgy TN1-997 Akhyar . I. Hasanuddin M. Ibrahim A. Farhan Z. Jalil Evaluation of cast defects in ship propeller of recycled aluminum alloy |
description |
The material used is recycled aluminum alloy. The ship’s propeller is cast through a steel mold. The macroporosity, misrun, and cold shut defects formed in the cast products of the ship’s propellers were observed for their location, geometric shape, and size. Defects are generally formed at the tip of the blade with various geometries and sizes, and shrinkage cavity defects are observed at the butt of the blade. No defects were found in the product when die mold was preheated. |
format |
article |
author |
Akhyar . I. Hasanuddin M. Ibrahim A. Farhan Z. Jalil |
author_facet |
Akhyar . I. Hasanuddin M. Ibrahim A. Farhan Z. Jalil |
author_sort |
Akhyar . |
title |
Evaluation of cast defects in ship propeller of recycled aluminum alloy |
title_short |
Evaluation of cast defects in ship propeller of recycled aluminum alloy |
title_full |
Evaluation of cast defects in ship propeller of recycled aluminum alloy |
title_fullStr |
Evaluation of cast defects in ship propeller of recycled aluminum alloy |
title_full_unstemmed |
Evaluation of cast defects in ship propeller of recycled aluminum alloy |
title_sort |
evaluation of cast defects in ship propeller of recycled aluminum alloy |
publisher |
Croatian Metallurgical Society |
publishDate |
2022 |
url |
https://doaj.org/article/53a3ea82a55f4709b15b36cbf78bdd55 |
work_keys_str_mv |
AT akhyar evaluationofcastdefectsinshippropellerofrecycledaluminumalloy AT ihasanuddin evaluationofcastdefectsinshippropellerofrecycledaluminumalloy AT mibrahim evaluationofcastdefectsinshippropellerofrecycledaluminumalloy AT afarhan evaluationofcastdefectsinshippropellerofrecycledaluminumalloy AT zjalil evaluationofcastdefectsinshippropellerofrecycledaluminumalloy |
_version_ |
1718407768523669504 |