Publisher Correction: Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries

The original version of this Article contained an error in the title, which was previously incorrectly given as ‘Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygene batteries’. The correct version states ‘lithium-oxygen’ in place of ‘lithium-oxygene...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Yoko Hase, Yasuhiro Komori, Takayoshi Kusumoto, Takashi Harada, Juntaro Seki, Tohru Shiga, Kazuhide Kamiya, Shuji Nakanishi
Formato: article
Lenguaje:EN
Publicado: Nature Portfolio 2019
Materias:
Q
Acceso en línea:https://doaj.org/article/54dd81504eef47abab64dc1c74c477fe
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:54dd81504eef47abab64dc1c74c477fe
record_format dspace
spelling oai:doaj.org-article:54dd81504eef47abab64dc1c74c477fe2021-12-02T15:36:06ZPublisher Correction: Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries10.1038/s41467-019-08964-x2041-1723https://doaj.org/article/54dd81504eef47abab64dc1c74c477fe2019-02-01T00:00:00Zhttps://doi.org/10.1038/s41467-019-08964-xhttps://doaj.org/toc/2041-1723The original version of this Article contained an error in the title, which was previously incorrectly given as ‘Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygene batteries’. The correct version states ‘lithium-oxygen’ in place of ‘lithium-oxygene’. This has been corrected in both the PDF and HTML versions of the Article.Yoko HaseYasuhiro KomoriTakayoshi KusumotoTakashi HaradaJuntaro SekiTohru ShigaKazuhide KamiyaShuji NakanishiNature PortfolioarticleScienceQENNature Communications, Vol 10, Iss 1, Pp 1-1 (2019)
institution DOAJ
collection DOAJ
language EN
topic Science
Q
spellingShingle Science
Q
Yoko Hase
Yasuhiro Komori
Takayoshi Kusumoto
Takashi Harada
Juntaro Seki
Tohru Shiga
Kazuhide Kamiya
Shuji Nakanishi
Publisher Correction: Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries
description The original version of this Article contained an error in the title, which was previously incorrectly given as ‘Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygene batteries’. The correct version states ‘lithium-oxygen’ in place of ‘lithium-oxygene’. This has been corrected in both the PDF and HTML versions of the Article.
format article
author Yoko Hase
Yasuhiro Komori
Takayoshi Kusumoto
Takashi Harada
Juntaro Seki
Tohru Shiga
Kazuhide Kamiya
Shuji Nakanishi
author_facet Yoko Hase
Yasuhiro Komori
Takayoshi Kusumoto
Takashi Harada
Juntaro Seki
Tohru Shiga
Kazuhide Kamiya
Shuji Nakanishi
author_sort Yoko Hase
title Publisher Correction: Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries
title_short Publisher Correction: Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries
title_full Publisher Correction: Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries
title_fullStr Publisher Correction: Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries
title_full_unstemmed Publisher Correction: Negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries
title_sort publisher correction: negative differential resistance as a critical indicator for the discharge capacity of lithium-oxygen batteries
publisher Nature Portfolio
publishDate 2019
url https://doaj.org/article/54dd81504eef47abab64dc1c74c477fe
work_keys_str_mv AT yokohase publishercorrectionnegativedifferentialresistanceasacriticalindicatorforthedischargecapacityoflithiumoxygenbatteries
AT yasuhirokomori publishercorrectionnegativedifferentialresistanceasacriticalindicatorforthedischargecapacityoflithiumoxygenbatteries
AT takayoshikusumoto publishercorrectionnegativedifferentialresistanceasacriticalindicatorforthedischargecapacityoflithiumoxygenbatteries
AT takashiharada publishercorrectionnegativedifferentialresistanceasacriticalindicatorforthedischargecapacityoflithiumoxygenbatteries
AT juntaroseki publishercorrectionnegativedifferentialresistanceasacriticalindicatorforthedischargecapacityoflithiumoxygenbatteries
AT tohrushiga publishercorrectionnegativedifferentialresistanceasacriticalindicatorforthedischargecapacityoflithiumoxygenbatteries
AT kazuhidekamiya publishercorrectionnegativedifferentialresistanceasacriticalindicatorforthedischargecapacityoflithiumoxygenbatteries
AT shujinakanishi publishercorrectionnegativedifferentialresistanceasacriticalindicatorforthedischargecapacityoflithiumoxygenbatteries
_version_ 1718386353038688256