Ageing of annealed and chemically strengthened glass
Eight 45-year-old naturally aged windows collected from two buildings in two different locations revealed surface characteristic bending strengths in the range of 38-54 MPa. An artificial ageing method by sandfall was developed to reproduce the weakest failure stresses among the naturally aged samp...
Guardado en:
Autor principal: | Xavier Gillon |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
Challenging Glass Conference
2020
|
Materias: | |
Acceso en línea: | https://doaj.org/article/58504a36b63844318b2c7fd151d7d5b0 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Recycled glass mixtures as cast glass components for structural applications, towards sustainability
por: Giulia Maria Anagni, et al.
Publicado: (2020) -
Rethinking the Cast Glass Mould.
por: Faidra Oikonomopoulou, et al.
Publicado: (2020) -
Residual Stress in Glass Components
por: L. Rammig
Publicado: (2016) -
Glass Structures & Engineering Papers
por: Challenging Glass
Publicado: (2016) -
Dynamic Behavior of Laminated Glass Plates
por: Claude Boutin, et al.
Publicado: (2020)