Investigation Produce of Particleboard with use of Bagasse and Haloxylon sp. in

In this study, for optimum using of agriculture residual and high density spices with a little consumption in the particleboard, the possibility of Haloxylon sp. use of the desert regions’ of Kerman and Bagasse available in the sugar came fields of Khuzestan province  was investigated. For this purp...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Ali Khalili gasht, Reza Mirza bighi azghandi
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2009
Materias:
Acceso en línea:https://doaj.org/article/686f3e28db2b4bbe8567cf98a676aab3
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:686f3e28db2b4bbe8567cf98a676aab3
record_format dspace
spelling oai:doaj.org-article:686f3e28db2b4bbe8567cf98a676aab32021-12-02T02:21:33ZInvestigation Produce of Particleboard with use of Bagasse and Haloxylon sp. in1735-09132383-112X10.22092/ijwpr.2009.117360https://doaj.org/article/686f3e28db2b4bbe8567cf98a676aab32009-03-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_117360_165b4cafbe6a659dca1d24512f033707.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XIn this study, for optimum using of agriculture residual and high density spices with a little consumption in the particleboard, the possibility of Haloxylon sp. use of the desert regions’ of Kerman and Bagasse available in the sugar came fields of Khuzestan province  was investigated. For this purpose of above mentioned raw materials with differente mixture percentage and with change effective agents in uniform particleboard such as particle moisture and press time, samples were made, and then were investigated mechanical and physical properties. For assessing the physical properties such as water absorption and mechanical properties such as rupture modulus, elasticity modulus and internal bonding were used according to the ASTM D-1037 standard. Results of this study showed that with increase amounts of Haloxylon sp. to 40%, rupture modulus and elasticity modulus increased and a great amount cause these strengths decreased. Also with increasing Haloxylon sp. amount to 60%, internal bonding values of boards increased and after this amount internal bonding decreased. With increased Haloxylon to 40%, water absorption in 2 & 24 hours decreased and then increased. Uniform particleboard rupture and elasticity modulus with increasing particle moisture to12% increased and then decreased. The Internal bonding with increasing moisture decreased. Optimum amount of moisture for absorption in 2 & 24 hours was 12%. The best press time for total strength in this study was 6 minutesAli Khalili gashtReza Mirza bighi azghandiRegional Information Center for Science and Technology (RICeST)articleHaloxylonBagassePRESS TIMEparticle moistureuniform particleboardoptimum amountForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 24, Iss 1, Pp 99-116 (2009)
institution DOAJ
collection DOAJ
language FA
topic Haloxylon
Bagasse
PRESS TIME
particle moisture
uniform particleboard
optimum amount
Forestry
SD1-669.5
spellingShingle Haloxylon
Bagasse
PRESS TIME
particle moisture
uniform particleboard
optimum amount
Forestry
SD1-669.5
Ali Khalili gasht
Reza Mirza bighi azghandi
Investigation Produce of Particleboard with use of Bagasse and Haloxylon sp. in
description In this study, for optimum using of agriculture residual and high density spices with a little consumption in the particleboard, the possibility of Haloxylon sp. use of the desert regions’ of Kerman and Bagasse available in the sugar came fields of Khuzestan province  was investigated. For this purpose of above mentioned raw materials with differente mixture percentage and with change effective agents in uniform particleboard such as particle moisture and press time, samples were made, and then were investigated mechanical and physical properties. For assessing the physical properties such as water absorption and mechanical properties such as rupture modulus, elasticity modulus and internal bonding were used according to the ASTM D-1037 standard. Results of this study showed that with increase amounts of Haloxylon sp. to 40%, rupture modulus and elasticity modulus increased and a great amount cause these strengths decreased. Also with increasing Haloxylon sp. amount to 60%, internal bonding values of boards increased and after this amount internal bonding decreased. With increased Haloxylon to 40%, water absorption in 2 & 24 hours decreased and then increased. Uniform particleboard rupture and elasticity modulus with increasing particle moisture to12% increased and then decreased. The Internal bonding with increasing moisture decreased. Optimum amount of moisture for absorption in 2 & 24 hours was 12%. The best press time for total strength in this study was 6 minutes
format article
author Ali Khalili gasht
Reza Mirza bighi azghandi
author_facet Ali Khalili gasht
Reza Mirza bighi azghandi
author_sort Ali Khalili gasht
title Investigation Produce of Particleboard with use of Bagasse and Haloxylon sp. in
title_short Investigation Produce of Particleboard with use of Bagasse and Haloxylon sp. in
title_full Investigation Produce of Particleboard with use of Bagasse and Haloxylon sp. in
title_fullStr Investigation Produce of Particleboard with use of Bagasse and Haloxylon sp. in
title_full_unstemmed Investigation Produce of Particleboard with use of Bagasse and Haloxylon sp. in
title_sort investigation produce of particleboard with use of bagasse and haloxylon sp. in
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 2009
url https://doaj.org/article/686f3e28db2b4bbe8567cf98a676aab3
work_keys_str_mv AT alikhaliligasht investigationproduceofparticleboardwithuseofbagasseandhaloxylonspin
AT rezamirzabighiazghandi investigationproduceofparticleboardwithuseofbagasseandhaloxylonspin
_version_ 1718402532048371712