Investigating the mechanical properties of wood flour/ polypropylene/ nanoclay composite
The effect of nanoclay and coupling agent contents on the mechanical properties of wood flour/ polypropylene/ nanoclay composites was investigated. Wood flour content was constant at 40%, maleic anhydride at two levels of 2 and 4% and nanoclay (Cloisite 30B) at four levels of 0, 1, 3 and 5% were use...
Guardado en:
Autores principales: | , , , |
---|---|
Formato: | article |
Lenguaje: | FA |
Publicado: |
Regional Information Center for Science and Technology (RICeST)
2013
|
Materias: | |
Acceso en línea: | https://doaj.org/article/68bb61322679491ba4be42186e4ef26d |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
id |
oai:doaj.org-article:68bb61322679491ba4be42186e4ef26d |
---|---|
record_format |
dspace |
spelling |
oai:doaj.org-article:68bb61322679491ba4be42186e4ef26d2021-12-02T04:16:21ZInvestigating the mechanical properties of wood flour/ polypropylene/ nanoclay composite1735-09132383-112X10.22092/ijwpr.2013.3112https://doaj.org/article/68bb61322679491ba4be42186e4ef26d2013-03-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_3112_02a23cf0ec91be312abb8d2705231632.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XThe effect of nanoclay and coupling agent contents on the mechanical properties of wood flour/ polypropylene/ nanoclay composites was investigated. Wood flour content was constant at 40%, maleic anhydride at two levels of 2 and 4% and nanoclay (Cloisite 30B) at four levels of 0, 1, 3 and 5% were used. The materials were mixed in an internal mixer at 180 o C, 60 rpm for 12 minutes, and then the specimens were fabricated by injection molding method. The mechanical properties such as tensile and flexural strength, flexural modulus and impact strength were measured. The nanoclay dispersion was examined by X-ray diffraction. The results indicated that the tensile and flexural strength, and the flexural modulus increased with increasing the nanoclay, but impact strength decreased. The tensile and flexural strength, flexural modulus increased as the compatibilizer content increased from 2 to 4%, but impact strength was decreased. The structural examination of the wood polymer nanocomposite with X-ray showed that nanoclay was distributed as intercalation structure in polymer matrix, and the d-spacing of layers were increased with increasing of nanoclay particles content.Habib alah Khademi eslamZahra YoosefniaEsmaeil GhasemiMohammad TalaeipoorRegional Information Center for Science and Technology (RICeST)articleWood Polymer CompositesCoupling agentNanoclayMECHANICAL PROPERTIESX-Ray DiffractionForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 28, Iss 1, Pp 153-168 (2013) |
institution |
DOAJ |
collection |
DOAJ |
language |
FA |
topic |
Wood Polymer Composites Coupling agent Nanoclay MECHANICAL PROPERTIES X-Ray Diffraction Forestry SD1-669.5 |
spellingShingle |
Wood Polymer Composites Coupling agent Nanoclay MECHANICAL PROPERTIES X-Ray Diffraction Forestry SD1-669.5 Habib alah Khademi eslam Zahra Yoosefnia Esmaeil Ghasemi Mohammad Talaeipoor Investigating the mechanical properties of wood flour/ polypropylene/ nanoclay composite |
description |
The effect of nanoclay and coupling agent contents on the mechanical properties of wood flour/ polypropylene/ nanoclay composites was investigated. Wood flour content was constant at 40%, maleic anhydride at two levels of 2 and 4% and nanoclay (Cloisite 30B) at four levels of 0, 1, 3 and 5% were used. The materials were mixed in an internal mixer at 180 o C, 60 rpm for 12 minutes, and then the specimens were fabricated by injection molding method. The mechanical properties such as tensile and flexural strength, flexural modulus and impact strength were measured. The nanoclay dispersion was examined by X-ray diffraction. The results indicated that the tensile and flexural strength, and the flexural modulus increased with increasing the nanoclay, but impact strength decreased. The tensile and flexural strength, flexural modulus increased as the compatibilizer content increased from 2 to 4%, but impact strength was decreased. The structural examination of the wood polymer nanocomposite with X-ray showed that nanoclay was distributed as intercalation structure in polymer matrix, and the d-spacing of layers were increased with increasing of nanoclay particles content. |
format |
article |
author |
Habib alah Khademi eslam Zahra Yoosefnia Esmaeil Ghasemi Mohammad Talaeipoor |
author_facet |
Habib alah Khademi eslam Zahra Yoosefnia Esmaeil Ghasemi Mohammad Talaeipoor |
author_sort |
Habib alah Khademi eslam |
title |
Investigating the mechanical properties of wood
flour/ polypropylene/ nanoclay composite |
title_short |
Investigating the mechanical properties of wood
flour/ polypropylene/ nanoclay composite |
title_full |
Investigating the mechanical properties of wood
flour/ polypropylene/ nanoclay composite |
title_fullStr |
Investigating the mechanical properties of wood
flour/ polypropylene/ nanoclay composite |
title_full_unstemmed |
Investigating the mechanical properties of wood
flour/ polypropylene/ nanoclay composite |
title_sort |
investigating the mechanical properties of wood
flour/ polypropylene/ nanoclay composite |
publisher |
Regional Information Center for Science and Technology (RICeST) |
publishDate |
2013 |
url |
https://doaj.org/article/68bb61322679491ba4be42186e4ef26d |
work_keys_str_mv |
AT habibalahkhademieslam investigatingthemechanicalpropertiesofwoodflourpolypropylenenanoclaycomposite AT zahrayoosefnia investigatingthemechanicalpropertiesofwoodflourpolypropylenenanoclaycomposite AT esmaeilghasemi investigatingthemechanicalpropertiesofwoodflourpolypropylenenanoclaycomposite AT mohammadtalaeipoor investigatingthemechanicalpropertiesofwoodflourpolypropylenenanoclaycomposite |
_version_ |
1718401374936367104 |