The effect of using Palm Flour in the Manufacture of pp-based wood-plastic Composite

In this research, the effect of the wood filler content and coupling agent (MAPP) on the physical and mechanical properties of Polypropylene reinforced with palm wood flour from the annual pruning of palm leaves (Shahani species) composite, were studied. For this purpose, the palm wood flour in thre...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Alireza Beiazyat, Laya Jamalirad, Hedayat alah Aminian, Sahab Hejazi
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2016
Materias:
Acceso en línea:https://doaj.org/article/6e9dd5e077ee42beb2cd895bf49be8bc
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:6e9dd5e077ee42beb2cd895bf49be8bc
record_format dspace
spelling oai:doaj.org-article:6e9dd5e077ee42beb2cd895bf49be8bc2021-12-02T02:36:29ZThe effect of using Palm Flour in the Manufacture of pp-based wood-plastic Composite1735-09132383-112X10.22092/ijwpr.2015.105771https://doaj.org/article/6e9dd5e077ee42beb2cd895bf49be8bc2016-03-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_105771_875e8e51b9365eea973c05b722dbdc7d.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XIn this research, the effect of the wood filler content and coupling agent (MAPP) on the physical and mechanical properties of Polypropylene reinforced with palm wood flour from the annual pruning of palm leaves (Shahani species) composite, were studied. For this purpose, the palm wood flour in three levels of 30%, 40%, 50% and two levels of Maleic anhydride grafted polypropylene 4% and 6% were used as variable factors. Then, the Physical and mechanical properties of samples, including thickness swelling after 2 and 24 hours of immersion in water, bending strength, bending modulus, tensile strength, tensile modulus and impact strength, were measured.The results showed that by increasing palm wood flour, the bending strength, tensile strength and impact strength were decreased but the thickness swelling, bending modulus, tensile modulus were increased. It was also found that by adding MAPP, thickness swelling, bending strength, bending modulus, tensile strength and tensile modulus were improved. The results revealed that at increased consumption of palm wood flour and adding coupling agent leads to improve quality of the interface and significant changes especially dimensional stability and MOE, are achieved.Alireza BeiazyatLaya JamaliradHedayat alah AminianSahab HejaziRegional Information Center for Science and Technology (RICeST)articleCompositePolypropylenePalm flourCoupling agentModulus of ElastisityForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 31, Iss 1, Pp 30-39 (2016)
institution DOAJ
collection DOAJ
language FA
topic Composite
Polypropylene
Palm flour
Coupling agent
Modulus of Elastisity
Forestry
SD1-669.5
spellingShingle Composite
Polypropylene
Palm flour
Coupling agent
Modulus of Elastisity
Forestry
SD1-669.5
Alireza Beiazyat
Laya Jamalirad
Hedayat alah Aminian
Sahab Hejazi
The effect of using Palm Flour in the Manufacture of pp-based wood-plastic Composite
description In this research, the effect of the wood filler content and coupling agent (MAPP) on the physical and mechanical properties of Polypropylene reinforced with palm wood flour from the annual pruning of palm leaves (Shahani species) composite, were studied. For this purpose, the palm wood flour in three levels of 30%, 40%, 50% and two levels of Maleic anhydride grafted polypropylene 4% and 6% were used as variable factors. Then, the Physical and mechanical properties of samples, including thickness swelling after 2 and 24 hours of immersion in water, bending strength, bending modulus, tensile strength, tensile modulus and impact strength, were measured.The results showed that by increasing palm wood flour, the bending strength, tensile strength and impact strength were decreased but the thickness swelling, bending modulus, tensile modulus were increased. It was also found that by adding MAPP, thickness swelling, bending strength, bending modulus, tensile strength and tensile modulus were improved. The results revealed that at increased consumption of palm wood flour and adding coupling agent leads to improve quality of the interface and significant changes especially dimensional stability and MOE, are achieved.
format article
author Alireza Beiazyat
Laya Jamalirad
Hedayat alah Aminian
Sahab Hejazi
author_facet Alireza Beiazyat
Laya Jamalirad
Hedayat alah Aminian
Sahab Hejazi
author_sort Alireza Beiazyat
title The effect of using Palm Flour in the Manufacture of pp-based wood-plastic Composite
title_short The effect of using Palm Flour in the Manufacture of pp-based wood-plastic Composite
title_full The effect of using Palm Flour in the Manufacture of pp-based wood-plastic Composite
title_fullStr The effect of using Palm Flour in the Manufacture of pp-based wood-plastic Composite
title_full_unstemmed The effect of using Palm Flour in the Manufacture of pp-based wood-plastic Composite
title_sort effect of using palm flour in the manufacture of pp-based wood-plastic composite
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 2016
url https://doaj.org/article/6e9dd5e077ee42beb2cd895bf49be8bc
work_keys_str_mv AT alirezabeiazyat theeffectofusingpalmflourinthemanufactureofppbasedwoodplasticcomposite
AT layajamalirad theeffectofusingpalmflourinthemanufactureofppbasedwoodplasticcomposite
AT hedayatalahaminian theeffectofusingpalmflourinthemanufactureofppbasedwoodplasticcomposite
AT sahabhejazi theeffectofusingpalmflourinthemanufactureofppbasedwoodplasticcomposite
AT alirezabeiazyat effectofusingpalmflourinthemanufactureofppbasedwoodplasticcomposite
AT layajamalirad effectofusingpalmflourinthemanufactureofppbasedwoodplasticcomposite
AT hedayatalahaminian effectofusingpalmflourinthemanufactureofppbasedwoodplasticcomposite
AT sahabhejazi effectofusingpalmflourinthemanufactureofppbasedwoodplasticcomposite
_version_ 1718402356220002304