Which is the Right Reference Surface Compression Value for Heat Treated Glass?
The paper correlates the data recorded in Stazione Sperimentale del Vetro, in many years. The aim is to define a correlation between the following parameters in heat treated glass: 1) bending strength tested according EN 1288-3 ; 2) fragmentation tested according relevant Standards [EN 1863-1 2004,...