Novel proton conducting core–shell PAMPS-PVBS@Fe2TiO5 nanoparticles as a reinforcement for SPEEK based membranes

Abstract In this study, new nanocomposite membranes from sulfonated poly (ether ether ketone) (SPEEK) and proton-conducting Fe2TiO5 nanoparticles are prepared by the solution casting method. Sulfonated core–shell Fe2TiO5 nanoparticles are synthesized by redox polymerization. Therefore, 4-Vinyl benze...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Parisa Salarizadeh, Mehran Javanbakht, Mohammad Bagher Askari, Khadijeh Hooshyari, Morteza Moradi, Hossein Beydaghi, Mohadese Rastgoo-Deylami, Morteza Enhessari
Formato: article
Lenguaje:EN
Publicado: Nature Portfolio 2021
Materias:
R
Q
Acceso en línea:https://doaj.org/article/7d32ab7784f74a63aa44b9013aaa2ae9
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
Descripción
Sumario:Abstract In this study, new nanocomposite membranes from sulfonated poly (ether ether ketone) (SPEEK) and proton-conducting Fe2TiO5 nanoparticles are prepared by the solution casting method. Sulfonated core–shell Fe2TiO5 nanoparticles are synthesized by redox polymerization. Therefore, 4-Vinyl benzene sulfonate (VBS) and 2-acrylamide-2-methyl-1-propane sulfonic acid (AMPS) are grafted on the surface of nanoparticles through radical polymerization. The different amounts of hybrid nanoparticles (PAMPS@Fe2TiO5 and PVBS@Fe2TiO5) are incorporated into the SPEEK matrix. The results show higher proton conductivity for all prepared nanocomposites than that of the SPEEK membrane. Embedding the sulfonated Fe2TiO5 nanoparticles into the SPEEK membrane improves proton conductivity by creating the new proton conducting sites. Besides, the nanocomposite membranes showed improved mechanical and dimensional stability in comparison with that of the SPEEK membrane. Also, the membranes including 2 wt% of PAMPS@Fe2TiO5 and PVBS@Fe2TiO5 nanoparticles indicate the maximum power density of 247 mW cm−2 and 226 mW cm−2 at 80 °C, respectively, which is higher than that of for the pristine membrane. Our prepared membranes have the potential for application in polymer electrolyte fuel cells.