Investigation of gluability and wettability properties of Medium Density Fiberboard produced using vine pruning fibers in combination with wood fibers

In this research, the effect of vine pruning fibers in combination with wood fibers on contact angel (wettability) and surface bond strength of medium density fiberboard was studied. One layer laboratory panels with a thickness of 15 mm and density of 650 Kg/Cm3 were produced. Variable factors were...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Fatemh Rezaei, Ali akbar Enayati
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2015
Materias:
Acceso en línea:https://doaj.org/article/8ab9364361074c05b72bbfbdd8fe48a3
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:8ab9364361074c05b72bbfbdd8fe48a3
record_format dspace
spelling oai:doaj.org-article:8ab9364361074c05b72bbfbdd8fe48a32021-12-02T00:20:29ZInvestigation of gluability and wettability properties of Medium Density Fiberboard produced using vine pruning fibers in combination with wood fibers1735-09132383-112X10.22092/ijwpr.2015.12919https://doaj.org/article/8ab9364361074c05b72bbfbdd8fe48a32015-06-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_12919_554d2a6eb997a6675eed9602b97b8aca.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XIn this research, the effect of vine pruning fibers in combination with wood fibers on contact angel (wettability) and surface bond strength of medium density fiberboard was studied. One layer laboratory panels with a thickness of 15 mm and density of 650 Kg/Cm3 were produced. Variable factors were vine pruning fibers content in three levels of 0/100, 30/70 and 60/40 by weight and press time in three levels of 4, 5 and 6 minutes. The wet ability and surface bond strength of panels were measured. Results showed that the contact angle of the boards was reduced when the vine pruning fibers content increased up to 60%. Press time had significant influence on wet ability of test panels. So that the contact angle was increased with increasing the press time up to 5 minutes. Whereas the contact angle was reduced when the press time of panels increased to 6 minutes. In addition, the results indicated that the sanding of panels caused a decrease of contact angle in the boards. Moreover the surface bond strength of panels were reduced with adding vine pruning fibers up to 30% whereas the panels produced using 60% vine pruning fibers showed stronger.Fatemh RezaeiAli akbar EnayatiRegional Information Center for Science and Technology (RICeST)articleMEDIUM DENSITY FIBERBOARDVine pruning fibersSurface bond strengthwettabilityContact angleForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 30, Iss 2, Pp 289-298 (2015)
institution DOAJ
collection DOAJ
language FA
topic MEDIUM DENSITY FIBERBOARD
Vine pruning fibers
Surface bond strength
wettability
Contact angle
Forestry
SD1-669.5
spellingShingle MEDIUM DENSITY FIBERBOARD
Vine pruning fibers
Surface bond strength
wettability
Contact angle
Forestry
SD1-669.5
Fatemh Rezaei
Ali akbar Enayati
Investigation of gluability and wettability properties of Medium Density Fiberboard produced using vine pruning fibers in combination with wood fibers
description In this research, the effect of vine pruning fibers in combination with wood fibers on contact angel (wettability) and surface bond strength of medium density fiberboard was studied. One layer laboratory panels with a thickness of 15 mm and density of 650 Kg/Cm3 were produced. Variable factors were vine pruning fibers content in three levels of 0/100, 30/70 and 60/40 by weight and press time in three levels of 4, 5 and 6 minutes. The wet ability and surface bond strength of panels were measured. Results showed that the contact angle of the boards was reduced when the vine pruning fibers content increased up to 60%. Press time had significant influence on wet ability of test panels. So that the contact angle was increased with increasing the press time up to 5 minutes. Whereas the contact angle was reduced when the press time of panels increased to 6 minutes. In addition, the results indicated that the sanding of panels caused a decrease of contact angle in the boards. Moreover the surface bond strength of panels were reduced with adding vine pruning fibers up to 30% whereas the panels produced using 60% vine pruning fibers showed stronger.
format article
author Fatemh Rezaei
Ali akbar Enayati
author_facet Fatemh Rezaei
Ali akbar Enayati
author_sort Fatemh Rezaei
title Investigation of gluability and wettability properties of Medium Density Fiberboard produced using vine pruning fibers in combination with wood fibers
title_short Investigation of gluability and wettability properties of Medium Density Fiberboard produced using vine pruning fibers in combination with wood fibers
title_full Investigation of gluability and wettability properties of Medium Density Fiberboard produced using vine pruning fibers in combination with wood fibers
title_fullStr Investigation of gluability and wettability properties of Medium Density Fiberboard produced using vine pruning fibers in combination with wood fibers
title_full_unstemmed Investigation of gluability and wettability properties of Medium Density Fiberboard produced using vine pruning fibers in combination with wood fibers
title_sort investigation of gluability and wettability properties of medium density fiberboard produced using vine pruning fibers in combination with wood fibers
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 2015
url https://doaj.org/article/8ab9364361074c05b72bbfbdd8fe48a3
work_keys_str_mv AT fatemhrezaei investigationofgluabilityandwettabilitypropertiesofmediumdensityfiberboardproducedusingvinepruningfibersincombinationwithwoodfibers
AT aliakbarenayati investigationofgluabilityandwettabilitypropertiesofmediumdensityfiberboardproducedusingvinepruningfibersincombinationwithwoodfibers
_version_ 1718403814197821440