Quantification of critical particle distance for mitigating catalyst sintering
Deactivation of supported metal catalysts via thermally induced sintering is a major concern in the catalysis community. Here, the authors demonstrate that enlarging particle distance to over the critical distance could suppress the particle coalescence greatly up to 900 °C.
Guardado en:
Autores principales: | Peng Yin, Sulei Hu, Kun Qian, Zeyue Wei, Le-Le Zhang, Yue Lin, Weixin Huang, Haifeng Xiong, Wei-Xue Li, Hai-Wei Liang |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
Nature Portfolio
2021
|
Materias: | |
Acceso en línea: | https://doaj.org/article/8eac23c06c724912b4a65d740575216e |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Recover the activity of sintered supported catalysts by nitrogen-doped carbon atomization
por: Huang Zhou, et al.
Publicado: (2020) -
Tracking the shape-dependent sintering of platinum–rhodium model catalysts under operando conditions
por: Uta Hejral, et al.
Publicado: (2016) -
The Dependence of CNT Aerogel Synthesis on Sulfur-driven Catalyst Nucleation Processes and a Critical Catalyst Particle Mass Concentration
por: Christian Hoecker, et al.
Publicado: (2017) -
Microstructural evolution during sintering of copper particles studied by laboratory diffraction contrast tomography (LabDCT)
por: S. A. McDonald, et al.
Publicado: (2017) -
Effects of different thermal sintering temperatures on pattern resistivity of printed silver ink with multiple particle sizes
por: Zhiheng Yu, et al.
Publicado: (2021)