Study on Static Strain Aging Kinetics of High-Carbon Steel Wires and Its Impact on High-Strength Steel Cords
Under quasi-static loading, an irregular failure mode of high-strength thin carbon steel cords were observed after low-temperature thermal aging. Character and kinetics of damage in such wire ropes highly depend on the plastic elongation of the steel wires, which is significantly modified by the str...
Guardado en:
Autores principales: | Tamás Bálint Mező, Péter Barkóczy |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
MDPI AG
2021
|
Materias: | |
Acceso en línea: | https://doaj.org/article/91e6236cfc0343a9bfef1b843b93e0fc |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Some complex intensification features of spheroidizing annealing of low carbon steel
por: G. Shvachych, et al.
Publicado: (2022) -
Cause analysis and improvement measures of steel-heaping in wire rods production
por: L. Zheng, et al.
Publicado: (2022) -
Behavior of composite self-compacting concrete (SCC) reinforced with steel wires from waste tires
por: Alpaslan-Köroğlu,Mehmet
Publicado: (2018) -
CMT-Based Wire Arc Additive Manufacturing Using 316L Stainless Steel (2): Solidification Map of the Multilayer Deposit
por: Jaewoong Park, et al.
Publicado: (2021) -
Tensile Behavior of High-Strength Stainless Steel Wire Rope (HSSSWR)-Reinforced ECC
por: Xinling Wang, et al.
Publicado: (2021)