Study on Static Strain Aging Kinetics of High-Carbon Steel Wires and Its Impact on High-Strength Steel Cords
Under quasi-static loading, an irregular failure mode of high-strength thin carbon steel cords were observed after low-temperature thermal aging. Character and kinetics of damage in such wire ropes highly depend on the plastic elongation of the steel wires, which is significantly modified by the str...
Enregistré dans:
Auteurs principaux: | Tamás Bálint Mező, Péter Barkóczy |
---|---|
Format: | article |
Langue: | EN |
Publié: |
MDPI AG
2021
|
Sujets: | |
Accès en ligne: | https://doaj.org/article/91e6236cfc0343a9bfef1b843b93e0fc |
Tags: |
Ajouter un tag
Pas de tags, Soyez le premier à ajouter un tag!
|
Documents similaires
-
Some complex intensification features of spheroidizing annealing of low carbon steel
par: G. Shvachych, et autres
Publié: (2022) -
Cause analysis and improvement measures of steel-heaping in wire rods production
par: L. Zheng, et autres
Publié: (2022) -
Behavior of composite self-compacting concrete (SCC) reinforced with steel wires from waste tires
par: Alpaslan-Köroğlu,Mehmet
Publié: (2018) -
CMT-Based Wire Arc Additive Manufacturing Using 316L Stainless Steel (2): Solidification Map of the Multilayer Deposit
par: Jaewoong Park, et autres
Publié: (2021) -
Tensile Behavior of High-Strength Stainless Steel Wire Rope (HSSSWR)-Reinforced ECC
par: Xinling Wang, et autres
Publié: (2021)