Boosting the catalysis of gold by O2 activation at Au-SiO2 interface

The development of sintering resistant supported Au catalysts with high activity still remains a challenge. Here the authors construct a Au-SiO2 interface by depositing SiO2 thin layer onto Au/TiO2 catalyst which shows very high activity in CO oxidation even after calcination at 800 °C.

Guardado en:
Detalles Bibliográficos
Autores principales: Yunlai Zhang, Junying Zhang, Bingsen Zhang, Rui Si, Bing Han, Feng Hong, Yiming Niu, Li Sun, Lin Li, Botao Qiao, Keju Sun, Jiahui Huang, Masatake Haruta
Formato: article
Lenguaje:EN
Publicado: Nature Portfolio 2020
Materias:
Q
Acceso en línea:https://doaj.org/article/9248a798c7ba4a5ea331aaf1d10f8106
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:9248a798c7ba4a5ea331aaf1d10f8106
record_format dspace
spelling oai:doaj.org-article:9248a798c7ba4a5ea331aaf1d10f81062021-12-02T14:42:16ZBoosting the catalysis of gold by O2 activation at Au-SiO2 interface10.1038/s41467-019-14241-82041-1723https://doaj.org/article/9248a798c7ba4a5ea331aaf1d10f81062020-01-01T00:00:00Zhttps://doi.org/10.1038/s41467-019-14241-8https://doaj.org/toc/2041-1723The development of sintering resistant supported Au catalysts with high activity still remains a challenge. Here the authors construct a Au-SiO2 interface by depositing SiO2 thin layer onto Au/TiO2 catalyst which shows very high activity in CO oxidation even after calcination at 800 °C.Yunlai ZhangJunying ZhangBingsen ZhangRui SiBing HanFeng HongYiming NiuLi SunLin LiBotao QiaoKeju SunJiahui HuangMasatake HarutaNature PortfolioarticleScienceQENNature Communications, Vol 11, Iss 1, Pp 1-10 (2020)
institution DOAJ
collection DOAJ
language EN
topic Science
Q
spellingShingle Science
Q
Yunlai Zhang
Junying Zhang
Bingsen Zhang
Rui Si
Bing Han
Feng Hong
Yiming Niu
Li Sun
Lin Li
Botao Qiao
Keju Sun
Jiahui Huang
Masatake Haruta
Boosting the catalysis of gold by O2 activation at Au-SiO2 interface
description The development of sintering resistant supported Au catalysts with high activity still remains a challenge. Here the authors construct a Au-SiO2 interface by depositing SiO2 thin layer onto Au/TiO2 catalyst which shows very high activity in CO oxidation even after calcination at 800 °C.
format article
author Yunlai Zhang
Junying Zhang
Bingsen Zhang
Rui Si
Bing Han
Feng Hong
Yiming Niu
Li Sun
Lin Li
Botao Qiao
Keju Sun
Jiahui Huang
Masatake Haruta
author_facet Yunlai Zhang
Junying Zhang
Bingsen Zhang
Rui Si
Bing Han
Feng Hong
Yiming Niu
Li Sun
Lin Li
Botao Qiao
Keju Sun
Jiahui Huang
Masatake Haruta
author_sort Yunlai Zhang
title Boosting the catalysis of gold by O2 activation at Au-SiO2 interface
title_short Boosting the catalysis of gold by O2 activation at Au-SiO2 interface
title_full Boosting the catalysis of gold by O2 activation at Au-SiO2 interface
title_fullStr Boosting the catalysis of gold by O2 activation at Au-SiO2 interface
title_full_unstemmed Boosting the catalysis of gold by O2 activation at Au-SiO2 interface
title_sort boosting the catalysis of gold by o2 activation at au-sio2 interface
publisher Nature Portfolio
publishDate 2020
url https://doaj.org/article/9248a798c7ba4a5ea331aaf1d10f8106
work_keys_str_mv AT yunlaizhang boostingthecatalysisofgoldbyo2activationatausio2interface
AT junyingzhang boostingthecatalysisofgoldbyo2activationatausio2interface
AT bingsenzhang boostingthecatalysisofgoldbyo2activationatausio2interface
AT ruisi boostingthecatalysisofgoldbyo2activationatausio2interface
AT binghan boostingthecatalysisofgoldbyo2activationatausio2interface
AT fenghong boostingthecatalysisofgoldbyo2activationatausio2interface
AT yimingniu boostingthecatalysisofgoldbyo2activationatausio2interface
AT lisun boostingthecatalysisofgoldbyo2activationatausio2interface
AT linli boostingthecatalysisofgoldbyo2activationatausio2interface
AT botaoqiao boostingthecatalysisofgoldbyo2activationatausio2interface
AT kejusun boostingthecatalysisofgoldbyo2activationatausio2interface
AT jiahuihuang boostingthecatalysisofgoldbyo2activationatausio2interface
AT masatakeharuta boostingthecatalysisofgoldbyo2activationatausio2interface
_version_ 1718389765510791168