Investigation on Neutral Sulfite Semi-Chemical Pulping of Reapseed (Canola) Residues

Neutral sulfite semi chemical pulping of Canola residues has been investigated. Canola residues collected from research farm at Agriculture and Natural Resources, University of Tehran, in Karaj. Chemical composition of Canola residues including cellulose, lignin, extractives soluble in ethanol-aceto...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Mohammad Ahmadi, Mohammad mehdi Faezipoor, Ahmad Jahan latibari, Sahab Hejazi
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2010
Materias:
Acceso en línea:https://doaj.org/article/a654c52a655f45d0b7d4ebbd3ed53ad5
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:a654c52a655f45d0b7d4ebbd3ed53ad5
record_format dspace
spelling oai:doaj.org-article:a654c52a655f45d0b7d4ebbd3ed53ad52021-12-02T02:13:42ZInvestigation on Neutral Sulfite Semi-Chemical Pulping of Reapseed (Canola) Residues1735-09132383-112X10.22092/ijwpr.2010.117272https://doaj.org/article/a654c52a655f45d0b7d4ebbd3ed53ad52010-03-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_117272_48273dc1d280bc37ed956219d2d4b808.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XNeutral sulfite semi chemical pulping of Canola residues has been investigated. Canola residues collected from research farm at Agriculture and Natural Resources, University of Tehran, in Karaj. Chemical composition of Canola residues including cellulose, lignin, extractives soluble in ethanol-acetone and ash were determined using relevant TAPPI standard test methods. Fiber dimensions of Canola residues were also measured. Then neutral sulfite semi chemical pulps were produced from Canola residues applying following conditions: Cooking time at 3 levels(20,40,60min),chemical charge at 5 levels(8,10,12,14,16 %), Cooking temperature was kept constant for all cooks at 175ċ , Na2SO3 to Na2CO3 ratio was 3:1,and liquor to Canola residues at 8:1. Each pulping was repeated tree times. At the end of each cooking, initial defibration was carried out using a laboratory disc refiner. Total yield before defibration and yield after defibration and screened yield were determined.  The highest yield (72%) was obtained at treatment combination of  and the lowest yield (58.7%) was in treatment of .Both factors, time and chemical charge, had significant effect on yield and increasing these two factors caused lower yield.Mohammad AhmadiMohammad mehdi FaezipoorAhmad Jahan latibariSahab HejaziRegional Information Center for Science and Technology (RICeST)articleCanola residuesNeutral Sulfite Semi Chemicaltotal yieldscreened yieldPULPForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 25, Iss 1, Pp 113-127 (2010)
institution DOAJ
collection DOAJ
language FA
topic Canola residues
Neutral Sulfite Semi Chemical
total yield
screened yield
PULP
Forestry
SD1-669.5
spellingShingle Canola residues
Neutral Sulfite Semi Chemical
total yield
screened yield
PULP
Forestry
SD1-669.5
Mohammad Ahmadi
Mohammad mehdi Faezipoor
Ahmad Jahan latibari
Sahab Hejazi
Investigation on Neutral Sulfite Semi-Chemical Pulping of Reapseed (Canola) Residues
description Neutral sulfite semi chemical pulping of Canola residues has been investigated. Canola residues collected from research farm at Agriculture and Natural Resources, University of Tehran, in Karaj. Chemical composition of Canola residues including cellulose, lignin, extractives soluble in ethanol-acetone and ash were determined using relevant TAPPI standard test methods. Fiber dimensions of Canola residues were also measured. Then neutral sulfite semi chemical pulps were produced from Canola residues applying following conditions: Cooking time at 3 levels(20,40,60min),chemical charge at 5 levels(8,10,12,14,16 %), Cooking temperature was kept constant for all cooks at 175ċ , Na2SO3 to Na2CO3 ratio was 3:1,and liquor to Canola residues at 8:1. Each pulping was repeated tree times. At the end of each cooking, initial defibration was carried out using a laboratory disc refiner. Total yield before defibration and yield after defibration and screened yield were determined.  The highest yield (72%) was obtained at treatment combination of  and the lowest yield (58.7%) was in treatment of .Both factors, time and chemical charge, had significant effect on yield and increasing these two factors caused lower yield.
format article
author Mohammad Ahmadi
Mohammad mehdi Faezipoor
Ahmad Jahan latibari
Sahab Hejazi
author_facet Mohammad Ahmadi
Mohammad mehdi Faezipoor
Ahmad Jahan latibari
Sahab Hejazi
author_sort Mohammad Ahmadi
title Investigation on Neutral Sulfite Semi-Chemical Pulping of Reapseed (Canola) Residues
title_short Investigation on Neutral Sulfite Semi-Chemical Pulping of Reapseed (Canola) Residues
title_full Investigation on Neutral Sulfite Semi-Chemical Pulping of Reapseed (Canola) Residues
title_fullStr Investigation on Neutral Sulfite Semi-Chemical Pulping of Reapseed (Canola) Residues
title_full_unstemmed Investigation on Neutral Sulfite Semi-Chemical Pulping of Reapseed (Canola) Residues
title_sort investigation on neutral sulfite semi-chemical pulping of reapseed (canola) residues
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 2010
url https://doaj.org/article/a654c52a655f45d0b7d4ebbd3ed53ad5
work_keys_str_mv AT mohammadahmadi investigationonneutralsulfitesemichemicalpulpingofreapseedcanolaresidues
AT mohammadmehdifaezipoor investigationonneutralsulfitesemichemicalpulpingofreapseedcanolaresidues
AT ahmadjahanlatibari investigationonneutralsulfitesemichemicalpulpingofreapseedcanolaresidues
AT sahabhejazi investigationonneutralsulfitesemichemicalpulpingofreapseedcanolaresidues
_version_ 1718402613033041920