The Effect of Deposited Dust on SCC and Crevice Corrosion of AISI 304L Stainless Steel in Saline Environment
Crevice corrosion has become an important issue of the safety of AISI 304L austenitic stainless steel canister when exposed to the chloride environments located in coastal areas. Moreover, dust deposited on the canister surface may enhance the corrosion effect of 304L stainless steel. In this work,...
Guardado en:
Autores principales: | Chun-Ping Yeh, Kun-Chao Tsai, Jiunn-Yuan Huang |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
MDPI AG
2021
|
Materias: | |
Acceso en línea: | https://doaj.org/article/ad6d00d0bb1e4af0a816fa4948d67dde |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Improvement of Erosion-Corrosion Behavior of AISI 420 Stainless Steel by Ion-Assisted Deposition ZrN Coatings
por: Yuntao Xi, et al.
Publicado: (2021) -
Investigation on the Correlation between Inclusions and High Temperature Urea Corrosion Behavior in Ferritic Stainless Steel
por: Xuelin Wang, et al.
Publicado: (2021) -
Study of Atmospheric Corrosion of Reinforcement Steel in Havana, Cuba
por: Castañeda,Abel, et al.
Publicado: (2014) -
Neurologic Dysfunction Associated With Mechanically Assisted Crevice Corrosion and Elevated Cobalt Ion Levels After Total Hip Arthroplasty
por: Brandon W. Yan, BA, et al.
Publicado: (2021) -
Improvement of Microhardness and Corrosion Resistance of Stainless Steel by Nanocomposite Coating
por: Hamid S. Mahdi, et al.
Publicado: (2017)