The article presents the results of a study of the wear resistance of sintered specimens from electroerosive powder of steel X13, obtained in butyl alcohol. The friction coefficient was 0.950, the width of the wear groove was 455.9 µm, the depth of the wear groove was 6 µm, the wear factor of the sa...