The effects of steaming time, press time and resin content on MDF properties

In this study Medium Density Fiberboard was produced from 4 year old Poplar clones (P.e. costanzo, P.e. 564.41, P.e. vernirubensis). Fibers length of P.e. costanzo, P.e. 564.41, P.e. vernirubensis were measured 805, 751 and 764 micron respectively. Also fibers diameter of these clones were determi...