Effects of Water Cooling on the Microstructure of Electron Beam Additive-Manufactured Ti-6Al-4V
The inferior mechanical properties of EBAM Ti-6Al-4V samples are due to the coarse columnar grains containing coarse lamellar structures. One can expect that water cooling of the build platform will increase the cooling rate of the molten pool during the build-up process, causing microstructure refi...
Guardado en:
Autores principales: | Alexey Panin, Sergey Martynov, Marina Kazachenok, Lyudmila Kazantseva, Alexander Bakulin, Svetlana Kulkova, Olga Perevalova, Elena Sklyarova |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
MDPI AG
2021
|
Materias: | |
Acceso en línea: | https://doaj.org/article/c68a1958fc444f4e98bfe3ca24613f1f |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Deformation Behavior of Wrought and EBAM Ti-6Al-4V under Scratch Testing
por: Artur Shugurov, et al.
Publicado: (2021) -
Experimental and numerical investigation of microstructure and evolution of TiNi Alloy/Q235 steel interfaces prepared by explosive welding
por: Ming Yang, et al.
Publicado: (2021) -
Characterization and thermal analysis of laser metal deposited γ-TiAl thin walls
por: B. Mallikarjuna, et al.
Publicado: (2021) -
Effect of cryogenic treatment on microstructure evolution and mechanical properties of high nitrogen plastic die steel
por: Congpeng Kang, et al.
Publicado: (2021) -
Effects of Ti on the forming, microstructure and mechanical properties of laser welded joints of SiCp/2A14 composites
por: Zhijia Hua, et al.
Publicado: (2021)