The Investigation of Acetylation and Anti-Oxidant Effect on Weathering of wood Plastic Composites By Means of FTIR and Color Metry (Color measurement)
In this study capability of acetylated poplar flour in manufacture of high density poly ethylene composite which expose to accelerated weathering, was investigated. The acetylation degrees at medium and zero (control) levels, use of anti- oxidant and duration of weathering were considered as variabl...
Guardado en:
Autores principales: | , , , , |
---|---|
Formato: | article |
Lenguaje: | FA |
Publicado: |
Regional Information Center for Science and Technology (RICeST)
2010
|
Materias: | |
Acceso en línea: | https://doaj.org/article/d0ab1287fe7f4e22b3aa35c14c084a7a |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
id |
oai:doaj.org-article:d0ab1287fe7f4e22b3aa35c14c084a7a |
---|---|
record_format |
dspace |
spelling |
oai:doaj.org-article:d0ab1287fe7f4e22b3aa35c14c084a7a2021-12-02T07:47:03ZThe Investigation of Acetylation and Anti-Oxidant Effect on Weathering of wood Plastic Composites By Means of FTIR and Color Metry (Color measurement)1735-09132383-112X10.22092/ijwpr.2010.117268https://doaj.org/article/d0ab1287fe7f4e22b3aa35c14c084a7a2010-03-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_117268_2e0ee75a60c543eb4bef89d90b178b82.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XIn this study capability of acetylated poplar flour in manufacture of high density poly ethylene composite which expose to accelerated weathering, was investigated. The acetylation degrees at medium and zero (control) levels, use of anti- oxidant and duration of weathering were considered as variables and their effects on discoloration and photodegradation of WPC were investigated. To determine treatments influence on changes and color fade resulting from weathering, samples were tested after o, 250, 2000 hours of weathering. The results indicated that application of acetylated wood flour in WPC can reduce about 25% of weathering discoloration in short time and about 17% in long time. Also it shows that as exposed time of weathering increase Anti oxidant loss its effect. Although in short time it can reduce 12% of weathering color changes. FTIR results show that after 2000 h of weathering all peaks samples had same decrease which mean none of the treatments were useful. But Anti oxidant can reduce depth of weathering.Pyvand DarabiHamideh AbdolzadehAli naghi KarimiSeeyed Ahmad MirshokraieKazem DoosthoseiniRegional Information Center for Science and Technology (RICeST)articleWood plastic compositesHigh Density Poly Ethylene/ Wood flourAcetylationAnti- OxidantWeathering and DiscolorationForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 25, Iss 1, Pp 70-79 (2010) |
institution |
DOAJ |
collection |
DOAJ |
language |
FA |
topic |
Wood plastic composites High Density Poly Ethylene/ Wood flour Acetylation Anti- Oxidant Weathering and Discoloration Forestry SD1-669.5 |
spellingShingle |
Wood plastic composites High Density Poly Ethylene/ Wood flour Acetylation Anti- Oxidant Weathering and Discoloration Forestry SD1-669.5 Pyvand Darabi Hamideh Abdolzadeh Ali naghi Karimi Seeyed Ahmad Mirshokraie Kazem Doosthoseini The Investigation of Acetylation and Anti-Oxidant Effect on Weathering of wood Plastic Composites By Means of FTIR and Color Metry (Color measurement) |
description |
In this study capability of acetylated poplar flour in manufacture of high density poly ethylene composite which expose to accelerated weathering, was investigated. The acetylation degrees at medium and zero (control) levels, use of anti- oxidant and duration of weathering were considered as variables and their effects on discoloration and photodegradation of WPC were investigated. To determine treatments influence on changes and color fade resulting from weathering, samples were tested after o, 250, 2000 hours of weathering. The results indicated that application of acetylated wood flour in WPC can reduce about 25% of weathering discoloration in short time and about 17% in long time. Also it shows that as exposed time of weathering increase Anti oxidant loss its effect. Although in short time it can reduce 12% of weathering color changes. FTIR results show that after 2000 h of weathering all peaks samples had same decrease which mean none of the treatments were useful. But Anti oxidant can reduce depth of weathering. |
format |
article |
author |
Pyvand Darabi Hamideh Abdolzadeh Ali naghi Karimi Seeyed Ahmad Mirshokraie Kazem Doosthoseini |
author_facet |
Pyvand Darabi Hamideh Abdolzadeh Ali naghi Karimi Seeyed Ahmad Mirshokraie Kazem Doosthoseini |
author_sort |
Pyvand Darabi |
title |
The Investigation of Acetylation and Anti-Oxidant Effect on Weathering of wood
Plastic Composites By Means of FTIR and Color Metry (Color measurement) |
title_short |
The Investigation of Acetylation and Anti-Oxidant Effect on Weathering of wood
Plastic Composites By Means of FTIR and Color Metry (Color measurement) |
title_full |
The Investigation of Acetylation and Anti-Oxidant Effect on Weathering of wood
Plastic Composites By Means of FTIR and Color Metry (Color measurement) |
title_fullStr |
The Investigation of Acetylation and Anti-Oxidant Effect on Weathering of wood
Plastic Composites By Means of FTIR and Color Metry (Color measurement) |
title_full_unstemmed |
The Investigation of Acetylation and Anti-Oxidant Effect on Weathering of wood
Plastic Composites By Means of FTIR and Color Metry (Color measurement) |
title_sort |
investigation of acetylation and anti-oxidant effect on weathering of wood
plastic composites by means of ftir and color metry (color measurement) |
publisher |
Regional Information Center for Science and Technology (RICeST) |
publishDate |
2010 |
url |
https://doaj.org/article/d0ab1287fe7f4e22b3aa35c14c084a7a |
work_keys_str_mv |
AT pyvanddarabi theinvestigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT hamidehabdolzadeh theinvestigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT alinaghikarimi theinvestigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT seeyedahmadmirshokraie theinvestigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT kazemdoosthoseini theinvestigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT pyvanddarabi investigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT hamidehabdolzadeh investigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT alinaghikarimi investigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT seeyedahmadmirshokraie investigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement AT kazemdoosthoseini investigationofacetylationandantioxidanteffectonweatheringofwoodplasticcompositesbymeansofftirandcolormetrycolormeasurement |
_version_ |
1718399186626412544 |