Post-breakage Tensile and Bending Response of Laminated Glass
Laminated glass, composed by glass plies sandwiching polymeric interlayers, can provide a safe post-glass breakage response, in compliance with the fail-safe approach used in the structural design. In fact, when glass breaks, shards remain attached to the polymer, preventing danger from falling mat...
Guardado en:
Autores principales: | Laura Galuppi, Gianni Royer Carfagni |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
Challenging Glass Conference
2018
|
Materias: | |
Acceso en línea: | https://doaj.org/article/d9309aa441a64df6bb2866c46e05826c |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Post Breakage Strength Testing for Overhead Laminated Glass
por: I. Stelzer, et al.
Publicado: (2016) -
Three-point bending test of laminated glass with PVB and EVA interlayers at elevated temperature
por: David Antolinc
Publicado: (2020) -
Influence of Temperature on Post-Breakage Behaviour of Laminated Glass Beams : Experimental Approach
por: D. Delincé, et al.
Publicado: (2010) -
Four-point bending tests of PVB double laminated glass panels – experiments and numerical analysis
por: Tomáš Hána, et al.
Publicado: (2020) -
Effects of Humidity and the Presence of Moisture at the Bond-line on the Interfacial Separation of Laminated Glass for Flat Glass Re-use
por: Rebecca Hartwell, et al.
Publicado: (2020)