Investigation of applying the old corrugated container (OCC) and aspen chips in particleboard production

In this study, aspen chips with OCC (Old Corrugated Container) were used in particleboard production and samples were prepared at two different levels of resin contents (%9 and %10) and three levels of combination: 1- %25 OCC +%75 aspen,       2- %50 OCC + %50 aspen,        3- %75 OCC +%25 aspen. In...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Amir Eshraghi, Habib alah Khademeslami, Amir Nourbakhsh, Behzad Bazyar, Mohammad Talaeipoor
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2010
Materias:
Acceso en línea:https://doaj.org/article/e3501a94b31e4b7d964d7d680f748cfd
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:e3501a94b31e4b7d964d7d680f748cfd
record_format dspace
spelling oai:doaj.org-article:e3501a94b31e4b7d964d7d680f748cfd2021-12-02T02:51:33ZInvestigation of applying the old corrugated container (OCC) and aspen chips in particleboard production1735-09132383-112X10.22092/ijwpr.2011.117156https://doaj.org/article/e3501a94b31e4b7d964d7d680f748cfd2010-03-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_117156_f2f7412d124a6fc1fc426bcb79a50c31.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XIn this study, aspen chips with OCC (Old Corrugated Container) were used in particleboard production and samples were prepared at two different levels of resin contents (%9 and %10) and three levels of combination: 1- %25 OCC +%75 aspen,       2- %50 OCC + %50 aspen,        3- %75 OCC +%25 aspen. Indeed in this study these two mentioned factors are variable and other factors such as press temperature: 165 ºC, press time: 5 minute, mat moisture %12, board density 0.75 g/cm3 and press pressure 30 kg/cm2 were constant. After the boards were manufactured according to DIN-68763 standard, were undergone different tests such as: bending strength, modulus of elasticity, internal bonding strength and thickness swelling after 2 & 24 hours immersion in water. The results indicate that second ratio(%50 OCC and %50 aspen chips) is proper for bending applications and the first ratio(%25 OCC and %75 aspen chips) is proper for tensile and thickness swelling applications. Therefore, applying the OCC more than %50 in manufacturing combination; result in decreasing the physical and mechanical properties. Moreover the results show that when the resin content increases, the board features improve.Amir EshraghiHabib alah KhademeslamiAmir NourbakhshBehzad BazyarMohammad TalaeipoorRegional Information Center for Science and Technology (RICeST)articlePARTICLEBOARDUREA-FORMALDEHYDEOld corrugated containerMODULUS OF RUPTUREMODULUS OF ELASTICITYInternal bondingThickness swellingForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 26, Iss 1, Pp 138-150 (2010)
institution DOAJ
collection DOAJ
language FA
topic PARTICLEBOARD
UREA-FORMALDEHYDE
Old corrugated container
MODULUS OF RUPTURE
MODULUS OF ELASTICITY
Internal bonding
Thickness swelling
Forestry
SD1-669.5
spellingShingle PARTICLEBOARD
UREA-FORMALDEHYDE
Old corrugated container
MODULUS OF RUPTURE
MODULUS OF ELASTICITY
Internal bonding
Thickness swelling
Forestry
SD1-669.5
Amir Eshraghi
Habib alah Khademeslami
Amir Nourbakhsh
Behzad Bazyar
Mohammad Talaeipoor
Investigation of applying the old corrugated container (OCC) and aspen chips in particleboard production
description In this study, aspen chips with OCC (Old Corrugated Container) were used in particleboard production and samples were prepared at two different levels of resin contents (%9 and %10) and three levels of combination: 1- %25 OCC +%75 aspen,       2- %50 OCC + %50 aspen,        3- %75 OCC +%25 aspen. Indeed in this study these two mentioned factors are variable and other factors such as press temperature: 165 ºC, press time: 5 minute, mat moisture %12, board density 0.75 g/cm3 and press pressure 30 kg/cm2 were constant. After the boards were manufactured according to DIN-68763 standard, were undergone different tests such as: bending strength, modulus of elasticity, internal bonding strength and thickness swelling after 2 & 24 hours immersion in water. The results indicate that second ratio(%50 OCC and %50 aspen chips) is proper for bending applications and the first ratio(%25 OCC and %75 aspen chips) is proper for tensile and thickness swelling applications. Therefore, applying the OCC more than %50 in manufacturing combination; result in decreasing the physical and mechanical properties. Moreover the results show that when the resin content increases, the board features improve.
format article
author Amir Eshraghi
Habib alah Khademeslami
Amir Nourbakhsh
Behzad Bazyar
Mohammad Talaeipoor
author_facet Amir Eshraghi
Habib alah Khademeslami
Amir Nourbakhsh
Behzad Bazyar
Mohammad Talaeipoor
author_sort Amir Eshraghi
title Investigation of applying the old corrugated container (OCC) and aspen chips in particleboard production
title_short Investigation of applying the old corrugated container (OCC) and aspen chips in particleboard production
title_full Investigation of applying the old corrugated container (OCC) and aspen chips in particleboard production
title_fullStr Investigation of applying the old corrugated container (OCC) and aspen chips in particleboard production
title_full_unstemmed Investigation of applying the old corrugated container (OCC) and aspen chips in particleboard production
title_sort investigation of applying the old corrugated container (occ) and aspen chips in particleboard production
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 2010
url https://doaj.org/article/e3501a94b31e4b7d964d7d680f748cfd
work_keys_str_mv AT amireshraghi investigationofapplyingtheoldcorrugatedcontaineroccandaspenchipsinparticleboardproduction
AT habibalahkhademeslami investigationofapplyingtheoldcorrugatedcontaineroccandaspenchipsinparticleboardproduction
AT amirnourbakhsh investigationofapplyingtheoldcorrugatedcontaineroccandaspenchipsinparticleboardproduction
AT behzadbazyar investigationofapplyingtheoldcorrugatedcontaineroccandaspenchipsinparticleboardproduction
AT mohammadtalaeipoor investigationofapplyingtheoldcorrugatedcontaineroccandaspenchipsinparticleboardproduction
_version_ 1718402132416135168