Reproducibility of small Ge2C6H10O7-added MgB2 bulks fabricated by ex situ Spark Plasma Sintering used in compound bulk magnets with a trapped magnetic field above 5 T
Abstract Bulk discs (20 mm diameter and 4.3 mm thickness) of MgB2 added with Ge2C6H10O7 were obtained by Spark Plasma Sintering. Six samples with composition MgB2(Ge2C6H10O7)0.0014 and one undoped sample were fabricated under similar conditions and were magnetically characterized in order to determi...