UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION

In this investigation feasibility of Beech slabs in particleboards production were prepared at three different contents resin of 9, 10, and 11 percent, press temperatures of 165°C and 175°C and hardener contents of 1.5 and 2.5 percent.Based on the DIN-68763 standard physical and mechanical propertie...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Amir Nourbakhsh, Abdolrahman Hosseinzadeh, Kazem Doosthosseini, Abolfazl Kargarfard, Mazyar Radkyan
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2005
Materias:
Acceso en línea:https://doaj.org/article/f03bb689807d4c34a00e565c79578456
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
Descripción
Sumario:In this investigation feasibility of Beech slabs in particleboards production were prepared at three different contents resin of 9, 10, and 11 percent, press temperatures of 165°C and 175°C and hardener contents of 1.5 and 2.5 percent.Based on the DIN-68763 standard physical and mechanical properties including MOR, MOE, IB, and thickness swelling (after 2 and 24 immersion in water) were tested.According to the factorial experimental design at completely random test was analysis. The potential utilization of Beech slabs residues in particleboard production including: resin content (11%), press time (6 min.), press temp. (175°C), and hardener contents (2.5%) were found.