INFLUENCE OF BATH TEMPERATURE AND PH VALUE ON PROPERTIES OF CHEMICALLY DEPOSITED CU4SNS4 THIN FILMS
Thin films of Cu4SnS4 semiconductors were prepared by chemical bath deposition technique in aqueous solutions. The effects of various bath temperatures (40, 50 and 60 °C) and pH values (pH 0.5, pH 1.0 and pH 1.5) on growth of films were reported. The structure and morphology characteristics of thin...
Guardado en:
Autores principales: | KASSIM,ANUAR, WEE TEE,TAN, SHARIF,ATAN MOHD, ABDULLAH,DZULKEFLY KUANG, HARON,MD. JELAS, MIN,HO SOON, SARAVANAN,NAGALINGAM |
---|---|
Lenguaje: | English |
Publicado: |
Sociedad Chilena de Química
2009
|
Materias: | |
Acceso en línea: | http://www.scielo.cl/scielo.php?script=sci_arttext&pid=S0717-97072009000400004 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
INFLUENCE OF BATH TEMPERATURE AND PH VALUE ON PROPERTIES OF CHEMICALLY DEPOSITED CU4SNS4 THIN FILMS
por: KASSIM,ANUAR, et al.
Publicado: (2009) -
Preparation of ZnTe thin films using chemical bath deposition technique
por: Iman Ahmed Younus, et al.
Publicado: (2020) -
Morphological and structural features of the CdxPb1−xS films obtained by CBD from ethylenediamine-citrate bath
por: A. D. Kutyavina, et al.
Publicado: (2021) -
Efficient n-i-p Monolithic Perovskite/Silicon Tandem Solar Cells with Tin Oxide via a Chemical Bath Deposition Method
por: Jiyeon Hyun, et al.
Publicado: (2021) -
Annealing effect on temperature stability and mechanical stress at the “CdxPb1−xS film – substrate” interface
por: L. N. Maskaeva, et al.
Publicado: (2020)