SILICON-CONTAINING AROMATIC POLY(ESTERS) DERIVED FROM BIS(4-CARBOXYPHENYL)METHYL-R-SILANE AND BIS(4-(HYDROXYMETHYL) PHENYL)METHYL-R-SILANE: SYNTHESIS, CHARACTERIZATION AND THERMAL STUDIES

This work describes the synthesis, characterization and thermal studies of poly(esters) (PEs) containing two Si atoms in the main chain, derived from aromatic diacids and aliphatic dialcohols in which the Si atom is bonded to methyl and/or ethyl groups. PEs were characterized by FT-IR and ¹H, 13C an...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: TAGLE,LUISH, TERRAZA,CLAUDIO A, PINO,LEONARDO I
Lenguaje:English
Publicado: Sociedad Chilena de Química 2012
Materias:
Acceso en línea:http://www.scielo.cl/scielo.php?script=sci_arttext&pid=S0717-97072012000200023
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
Descripción
Sumario:This work describes the synthesis, characterization and thermal studies of poly(esters) (PEs) containing two Si atoms in the main chain, derived from aromatic diacids and aliphatic dialcohols in which the Si atom is bonded to methyl and/or ethyl groups. PEs were characterized by FT-IR and ¹H, 13C and 29Si spectroscopy and the results were in agreement with the proposed structures. Poly(esters) were soluble in polar aprotic solvents, such as DMSO and DMF, and acetone, and partially soluble in ethanol. The inherent viscosity and glass transition and thermal decomposition temperatures, h inh, Tg and TDT respectively, were determined. These results showed that PE-2 and PE-4, derived from the dialcohol with the -Si(CH3)(CH2CH3)- moiety as central element, had the larger values of h inh, Tg, TDT and the residual weight after heating at 900 °C, indicating that the specific structure of aliphatic dialcohols control the reaction.