Chemical changes of heat treated pine and eucalypt wood monitored by FTIR

A hardwood, Eucalyptus globulus Labill., and a softwood Pinus pinaster Aiton., were heat treated at temperatures between 170 and 210ºC in an oven and in an autoclave. The samples were pre-extracted with dichloromethane, ethanol and water and ground prior to Fourier Transform Infrared (FTIR) spectros...