Evaluation of physical and mechanical properties of wild cherry wood heat-treated using the thermowood process

The aim of this study is to determine the change of some physical properties (oven-dry density, weight loss, swelling and anti-swelling efficiency) and mechanical properties (compression strength parallel to grain, bending strength, modulus of elasticity in bending, janka-hardness (cross-section, ra...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Korkut,Süleyman, Aytin,Ayhan
Lenguaje:English
Publicado: Universidad del Bío-Bío 2015
Materias:
Acceso en línea:http://www.scielo.cl/scielo.php?script=sci_arttext&pid=S0718-221X2015000100018
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
Descripción
Sumario:The aim of this study is to determine the change of some physical properties (oven-dry density, weight loss, swelling and anti-swelling efficiency) and mechanical properties (compression strength parallel to grain, bending strength, modulus of elasticity in bending, janka-hardness (cross-section, radial, tangential), impact bending strength and tension strength perpendicular to grain) of wild cherry woods after heat treatment under different durations. Specimens are exposed to temperature levels of 212°C for time spans of 1,5 and 2,5 h. Based on the findings in this study, the results showed that oven-dry density, swelling, compression strength parallel to grain, bending strength, modulus of elasticity in bending, janka-hardness (Cross-section, Radial, Tangential), impact bending strength and tension strength perpendicular to grain values decreased with increasing treatment time.