Thermogravimetric analysis of anningre tannin resin

Three formulations of aningre tannin resins containing in order the paraformaldehyde powder, hexamethylenetetramine and aqueous glyoxal as hardeners were developed. Their thermogravimetric analysis have shown that they begin to decompose respectively from 135°C, 145°C and 140°C. About 24%, 40% and 3...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Konai,Noel, Raidandi,Danwe, Pizzi,Antonio, Girods,Pierre, Lagel,Marie-Christine, Kple,Melhyas
Lenguaje:English
Publicado: Universidad del Bío-Bío 2016
Materias:
Acceso en línea:http://www.scielo.cl/scielo.php?script=sci_arttext&pid=S0718-221X2016000200002
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:scielo:S0718-221X2016000200002
record_format dspace
spelling oai:scielo:S0718-221X20160002000022016-05-13Thermogravimetric analysis of anningre tannin resinKonai,NoelRaidandi,DanwePizzi,AntonioGirods,PierreLagel,Marie-ChristineKple,Melhyas Aningre tannin resins decomposition residues hardeners thermogravimetric analysis temperature thermomechanical analysis Three formulations of aningre tannin resins containing in order the paraformaldehyde powder, hexamethylenetetramine and aqueous glyoxal as hardeners were developed. Their thermogravimetric analysis have shown that they begin to decompose respectively from 135°C, 145°C and 140°C. About 24%, 40% and 39 % solid residues of their initial masses exist at the end of the analysis. Thermomechanical analysis has shown that the formulation containing paraformaldehyde powder as hardener has the best rigidity and the worst contains the hexamethylenetetramine. All formulations have different thermal degradation, differences were more significant between 400 and 900°C. The decomposition of hardeners become more significant from 400°C.info:eu-repo/semantics/openAccessUniversidad del Bío-BíoMaderas. Ciencia y tecnología v.18 n.2 20162016-04-01text/htmlhttp://www.scielo.cl/scielo.php?script=sci_arttext&pid=S0718-221X2016000200002en10.4067/S0718-221X2016005000022
institution Scielo Chile
collection Scielo Chile
language English
topic Aningre tannin resins
decomposition
residues hardeners
thermogravimetric analysis
temperature
thermomechanical analysis
spellingShingle Aningre tannin resins
decomposition
residues hardeners
thermogravimetric analysis
temperature
thermomechanical analysis
Konai,Noel
Raidandi,Danwe
Pizzi,Antonio
Girods,Pierre
Lagel,Marie-Christine
Kple,Melhyas
Thermogravimetric analysis of anningre tannin resin
description Three formulations of aningre tannin resins containing in order the paraformaldehyde powder, hexamethylenetetramine and aqueous glyoxal as hardeners were developed. Their thermogravimetric analysis have shown that they begin to decompose respectively from 135°C, 145°C and 140°C. About 24%, 40% and 39 % solid residues of their initial masses exist at the end of the analysis. Thermomechanical analysis has shown that the formulation containing paraformaldehyde powder as hardener has the best rigidity and the worst contains the hexamethylenetetramine. All formulations have different thermal degradation, differences were more significant between 400 and 900°C. The decomposition of hardeners become more significant from 400°C.
author Konai,Noel
Raidandi,Danwe
Pizzi,Antonio
Girods,Pierre
Lagel,Marie-Christine
Kple,Melhyas
author_facet Konai,Noel
Raidandi,Danwe
Pizzi,Antonio
Girods,Pierre
Lagel,Marie-Christine
Kple,Melhyas
author_sort Konai,Noel
title Thermogravimetric analysis of anningre tannin resin
title_short Thermogravimetric analysis of anningre tannin resin
title_full Thermogravimetric analysis of anningre tannin resin
title_fullStr Thermogravimetric analysis of anningre tannin resin
title_full_unstemmed Thermogravimetric analysis of anningre tannin resin
title_sort thermogravimetric analysis of anningre tannin resin
publisher Universidad del Bío-Bío
publishDate 2016
url http://www.scielo.cl/scielo.php?script=sci_arttext&pid=S0718-221X2016000200002
work_keys_str_mv AT konainoel thermogravimetricanalysisofanningretanninresin
AT raidandidanwe thermogravimetricanalysisofanningretanninresin
AT pizziantonio thermogravimetricanalysisofanningretanninresin
AT girodspierre thermogravimetricanalysisofanningretanninresin
AT lagelmariechristine thermogravimetricanalysisofanningretanninresin
AT kplemelhyas thermogravimetricanalysisofanningretanninresin
_version_ 1714202622462787584