Mechanical parameters of thermally modified ash wood determined on compression in tangential direction
Abstract: Mechanical parameters of ash wood (Fraxinus excelsior) subjected to compression in tangential direction, before and after its thermal modification and measured at the moisture content close to the equilibrium moisture content of wood used inside and outside the house, (4 and 12%) were comp...
Guardado en:
Autores principales: | Moliński,Waldemar, Roszyk,Edward, Jabłoński,Aleksander, Puszyński,Jakub, Cegieła,Janusz |
---|---|
Lenguaje: | English |
Publicado: |
Universidad del Bío-Bío
2018
|
Materias: | |
Acceso en línea: | http://www.scielo.cl/scielo.php?script=sci_arttext&pid=S0718-221X2018000221001 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Mechanical parameters of thermally modified ash wood determined by compression in radial direction
por: Moliński,Waldemar, et al.
Publicado: (2016) -
PHENOLICS COMPOSITION, ANTIOXIDANT AND CORROSION INHIBITION EFFICIENCY, CAPACITY OF F raxinus Excelsior EXTRACTS
por: Samra,Amamra, et al.
Publicado: (2021) -
Transformation of European Ash (<i>Fraxinus excelsior</i> L.) Callus as a Starting Point for Understanding the Molecular Basis of Ash Dieback
por: Anna Hebda, et al.
Publicado: (2021) -
Variation in Mechanical Properties within Individual Annual Rings in the Resonance Spruce Wood (Picea abies (L.) Karst.)
por: Waldemar Moliński, et al.
Publicado: (2014) -
RELATIONSHIP BETWEEN GLOBAL AND LOCAL MODULUS OF ELASTICITY IN BEAMS OF ARGENTINEAN Eucalyptus grandis
por: PITER,J.C, et al.
Publicado: (2003)