Nanostructured laminar tungsten alloy with improved ductility by surface mechanical attrition treatment

Abstract A nanostructured laminar W-La2O3 alloy (WL10) with improved ductility was prepared using a surface mechanical attrition treatment (SMAT). φ1.5 mm ZrO2 WL10 balls subjected to SMAT (called φ1.5 mm ZrO2 ball SMATed WL10) samples possess the best surface profile and excellent integrated mechan...